Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ISO 294-4 |
Polyplastic Armlen® PP GF 20-1EX Polypropylene Copolymer, 20% Glass Fiber Information provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycoloy® RCM6123 PC+ABS (Asia Pacific) Cycoloy* RCM6123 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 503R PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | ASTM D955 |
PolyOne Edgetek® PC-20GF/000 Polycarbonate (PC) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp DFP22 PC LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D955 |
PolyOne Edgetek® AS-10GF/000 NATURAL Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | Internal Method |
Solvay Specialty Polymers Ixef® 1002 Polyarylamide (PARA)
(Unverified Data**) Ixef 1002 is a 30% glass-fiber reinforced, general purpose polyarylamide compound which exhibits high strength and rigidity, outstanding surface finish, and excellent creep resistance. - Black: Ixef.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | |
Idemitsu Kosan Xarec® WA 210 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified, Improved Mold Release. Used in Automotive and Industrial applications. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D995 |
Kotec Carbotex KGN-30MRA Polycarbonate, Flame Retardant, 30% Glass Fiber Reinforced Features: Glass fiber 30% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0040 cm/cm | 0.0015 - 0.0040 in/in | |
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+PS (Asia Pacific) GR 30%. 275F (135C) DTUL. UL94 V-1 rated. Halogen free flame retardant. For electrical construction market. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RFL369 PA6.6 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFL369 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Flame Retardant. Added features include: Flame Retardant, internally lubricated |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features include: Exceptional Processing, Non-Brominated & Non-Chlorinated Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC LNP* Thermocomp* DF004RXP is a compound based on Polycarbonate resin containing 20% Glass Fiber. Some light color grades may have lower impact data than natural and black. Added features include: .. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP JX97000 PES (Europe-Africa-Middle East) LNP* Thermocomp* JX97000 is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Mold Release. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0040 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® TF-0930 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. Noryl GFN1520V cust spec 1977 has been certified for potable water applications up to 85C in Europe and No.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GFN3 PPE+PS PPE+PS blend. 30% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF25-66 XE-N 25% Glass Fiber Reinforced, Engineering Grade Nylon 66 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRGF25/15 42H-N1/WE1705-N1 40% Mineral/Glass Fiber Reinforced Nylon 6 Description: Mineral/Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 4.00 mm |
0.0020 - 0.0040 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA66 30Y D61 PA66, Carbon Fiber Filled, Injection Molded Star L PA66 30Y D51 is a PTFE/Silicone Oil Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 4.00 mm |
0.0020 - 0.0040 in/in @Thickness 0.157 in |
ISO 294 |
Eurostar Starflam PF0047E PA6, 20% Glass Filled, Injection Molded Starflam PF0047E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as EXCP4009)Information provided by Polymer Tech.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL FE1410PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1410PW resin is a blend of polyphenylene Oxide (PPO) and polystyrene (PS) resin that contains 10% glass reinforcement. The resin is suitable for injection molding. Noryl FE1410PW resin has .. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS+GF20%, Halogen Free Flame Retardant, High StiffnessApplication: E&E (Housing, OA Frame)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 65997-17-3Information provi.. |