Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 0250 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 0826 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ASTM D955 and ISO 294-4 |
Ravago Manufacturing Americas Hylon® N1200STHL BK Nylon 6/6 Available in North America Additive: Heat Stabilizer and Lubricant Features: Lubricated, Good Toughness and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B7500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standar.. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm @Thickness 3.17 mm |
0.017 - 0.021 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat StabilizedRoHS CompliantAuto Specifications: GM GMP.PA66.074 Color: BlackF.. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.020 cm/cm @Thickness 3.20 mm |
0.017 - 0.020 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | |
LATI Latiohm 75/4-10 CNT PBT Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | |
LATI Latishield 75/4-10A PBT, Steel Fiber Reinforced EMI shielding product based on Polybutylene Terephthalate (PBT). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.018 cm/cm @Time 86400 sec |
0.017 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® ABS 03106 MB Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.022 cm/cm | 0.017 - 0.022 in/in | |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA) Amodel® AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40.. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA12 Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 8807105Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.023 cm/cm @Thickness 3.20 mm |
0.017 - 0.023 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® VAC3003 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Time 86400 sec |
0.017 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON MX12407C PP LNP* STAT-KON* MX12407C is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 GB15 15% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 15% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6 TL10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (10%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | 24 hours + 30 min at 93°C |
Teknor Apex TEKRON® 4300LM-P86-1 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22LHI3 XE-NBK1 Impact Modified Engineering Nylon 66 Description: Impact Modified Engineering Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal.. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 4.00 mm |
0.017 in/in @Thickness 0.157 in |
E2P method |
Eurostar Staramide P1000J5 PA6, Impact Modified, Injection Molded Staramide P1000J5 is a Low Temperature Impact Modified, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | Eurotec |
Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, improved impact, heat stabilized, black Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
Clariant Renol 6253-L UV Nylon 6, High Impact, Lubricated, UV Stabilized Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ISO 2577 |
BASF Ultraform® N2720 M210 POM Description: Is a POM, product with increased stiffness and strength as well as good wear characteristics, used, for instance, for sliding chains and conveyor systems.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | Sheet |
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermotuf P1000J5 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* P1000J5 is a compound based on PA 6 resin containing Impact Modifier.
Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ISO 294-4 |
DuPont Performance Polymers Crastin® S610SF NC010 PBT
(Unverified Data**) Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Informati.. |