Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 2.00 mm |
0.016 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4 |
Akro-Plastic Akromid® S31 (3484) PA 6.10 Conditioned
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers CPP-0107 Polypropylene Homopolymer Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers PPC-320 Polypropylene, Impact Modified Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Elastoblend® PA6 IM 407 L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Elastoblend® PA6 IM 409 L MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PBT 613 RD Availability: North AmericaForms: PelletsUL File Number: E157318Appearance: Red8661111Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® POM CO 0150 S Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6/12 05007 Nylon 612 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PBT GB30 TL15 30% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® POM CO X Acetal Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Plastiblend® POM CO UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp M10009A PP (Europe-Africa-Middle East) LNP* STARFLAM* M10009A is a compound based on Polypropylene resin, containing Flame Retardant. Added features include : Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Time 86400 sec |
0.016 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RZ006S PA 66 (Asia Pacific) LNP* Thermocomp* RZ006S is a compound based on Nylon 66 resin containing Milled Glass. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PA (Europe-Africa-Middle East) NORYL GTX918W is an unfilled global grade, which offers an excellent combination of processability and heat resistance. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® PP CO E FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant and CopolymerProcessing Method: ExtrudedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PBT 0158 S Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® AZ 3 PA66 Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET
(Unverified Data**) 82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Sorona® 3301 BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight w.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® FG53 NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | Eurotec |
Eurotec® Tecodur® PB50 NL PBT, unfilled, natural, high viscosity Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 2577 |
BASF Ultramid® S3K Balance PA 610 (Conditioned) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 2577 |
BASF Ultramid® S3K Balance PA 610 (Dry) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers PPC-310 Polypropylene, Impact Modified Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22LH-WBK Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |