Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
PolyOne LubriOne™ PC-000/05T-2S Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | ASTM D955 |
PolyOne Nymax™ GMF 600 A 40 Natural Polyamide 6 (Nylon 6) The Nymax® 600 Series of mineral-reinforced nylon 6 compounds have been specifically developed to provide an excellent balance of physical property performance and durability, with improved surface.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycolac® EX58F ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | Euronil |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® FST9436 PC Copolymer Medium viscosity opaque, low smoke, and OSU 65/65 compliant PC Copolymer |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.012 cm/cm | 0.0060 - 0.012 in/in | ASTM D955 |
PolyOne Dynaflex™ G7970-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® SLX2571T PC Copolymer (Europe-Africa-Middle East) Transparent weatherable PC copolymer for blowmolding/extrusion. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 925AU PC (Asia Pacific) Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 955 PC Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.011 cm/cm | 0.0060 - 0.011 in/in | ASTM D955 |
PolyOne Dynaflex™ G7980-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7980-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4 |
Mitsubishi Xantar® 19 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers PC-1410FD Polycarbonate, FDA Compliant, Injection/Extrusion Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers PC-1418 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4 |
Mitsubishi Xantar® MX 2042 FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | |
Solvay TECHNYL® A 218 V25 Black 21NHFE PA66, 25% glass fiber, DRY Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics PREVEX W20 PPE+PS (Asia Pacific) Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | |
Solvay TECHNYL® R AR 130/GF Nylon 66, 30% glass fiber, DRY Description: TECHNYL® AR 130/GF is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. It contains recycled raw materials. This product is available in bla.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm @Thickness 3.20 - 4.60 mm |
0.0060 - 0.0090 in/in @Thickness 0.126 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm @Time 86400 sec |
0.0060 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP KF005 Acetal Copolymer LNP THERMOCOMP* KF005 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Time 86400 sec |
0.0060 - 0.0080 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF003AXH PA 66 LNP* THERMOCOMP* RF003AXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.019 cm/cm | 0.0060 - 0.019 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Asia Pacific) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PPO534 PPE+HIPS (Asia Pacific) PPO/PS unfilled high heat |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Time 86400 sec |
0.0060 - 0.0080 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP TF002 PU LNP* THERMOCOMP* TF002 is a compound based on Polyurethane resin containing 10% Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Statiblend® PPS GF23 IM BK 23% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 23% Filler by WeightAdditive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 925U PC Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additi.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 6.40 mm |
0.0060 - 0.0080 in/in @Thickness 0.252 in |
SABIC Method |
SABIC Innovative Plastics NORYL FN150X PPE+PS Improved reliability and productivity. Thin wall capability. UL94 V-0/5VA rated. All data at 20% weight reduction and 0.250"" wall. |