| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.020 - 0.025 cm/cm | 0.020 - 0.025 in/in | ISO 294-4 |
| Premix Thermoplastics PRE-ELEC® 12-000 PRE-ELEC 12-000 is a conductive thermoplastic compound based on a polyacetal copolymer. Conductivity is achieved by using special carbon black. In addition to a low resistivity PRE-ELEC 12-000 has a.. |
|||
| Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | ASTM D955 |
| Alcoa KAMA Petwich-PET 4300 Petwich-PET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Recycled contentSi.. |
|||
| Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | LATI |
| LATI LATILUB 73/13-20ST Polyoxymethylene Base (POM), 20% Mixed PTFE/Silicone Self Lubricating Plastic
(discon Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
| Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
| Kolon KOCETAL® K900 Standard Grade Acetal Resin Very low viscosity grade. Applications: Thin and large products.Information provided by API-Kolon. |
|||
| Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
| Multibase Multi-Flex® RP 6568 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good General PurposeOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInfor.. |
|||
| Linear Mold Shrinkage | 0.020 - 0.030 cm/cm @Thickness 3.17 mm |
0.020 - 0.030 in/in @Thickness 0.125 in |
ASTM D955 |
| Fiberfil® J-60/15/MI/20 Polypropylene Homopolymer, 35% Glass/mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
| Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | |
| Shin-Etsu Silicones LIMSâ„¢ KE1950-30A/B Elastomer KE-1950-30 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
| Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | |
| Teknor Apex TEKBOND® MP 1726 UVF Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
| Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | |
| Teknor Apex TEKBOND® MP 1728 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
| Linear Mold Shrinkage | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | |
| Polyram RamTal PM8427 Acetal, Impact modified Impact modified polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
| Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
| Daikin POLYFLON M-111 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with extremely smooth and fine surface. Suited to making packing and gaskets since moldings have an especially go.. |
|||
| Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
| Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic compression molding.Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding proces.. |
|||
| Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
| Daikin POLYFLON M-393 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding, automatic compression molding, and ram extrusion.Features: Maximum emphasis given to ease of handling during molding. Used when molded arti.. |
|||
| Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
| Daikin POLYFLON MG-1241 PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder 20% glass fiber and 5% graphite filled. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (e.g. piston rings, bearing pads, and packings)Inform.. |
|||
| Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
| Daikin POLYFLON MG-2060 PTFE 30% Graphite Filled Molding Powder 30% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki.. |
|||
| Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
| Daikin POLYFLON MG-6030F PTFE 15% Carbon Fiber Filled Molding Powder, High Apparent Density, Free Flow 15% carbon fiber filled. High apparent density and free-flowing properties. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechan.. |
|||
| Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM Data; MD |
| BASF Ultraform H 2320 006 Q600 POM Ultraform H2320 006 is a high-molecular-weight grade of POM for injection molding. It conforms to FDA requirements of 21 CFR 177.2470. |
|||
| Linear Mold Shrinkage | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
ISO 294-4 |
| Ascend Performance Materials Vydyne® 65A Nylon 66, General Purpose, intermediate viscosity, DAM Vydyne® 65A is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding extrusion and compounding applications. It is available in natural color only. Vydyne 65A resin offers h.. |
|||