| Category | Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded |
| Manufacturer | Daikin Industries |
| Trade Name | POLYFLON |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Daikin POLYFLON F-302 PTFE Fine Powder.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
| Bulk Density | 0.475 g/cc | 0.0172 lb/in³ | |
| Water Absorption | 0.00 % @Thickness 8.50 mm, Time 86400 sec |
0.00 % @Thickness 0.335 in, Time 24.0 hour |
ASTM D570 |
| Particle Size | 500 µm | 500 µm | |
| Viscosity | 1.00e+13 - 1.00e+15 cP @Temperature 340 - 380 °C |
1.00e+13 - 1.00e+15 cP @Temperature 644 - 716 °F |
Melt viscosity |
| Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
| Deformation | 5.0 % | 5.0 % | 6.7 MPa load, at 100°C, 24 hrs; ASTM D621 |
| 7.0 % | 7.0 % | 13.7 MPa load, at 25°C, 24 hrs; ASTM D621 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 50 - 65 | 50 - 65 | |
| Tensile Strength at Break | 20.0 - 45.0 MPa | 2900 - 6530 psi | ASTM D638 |
| Elongation at Break | 200 - 450 % | 200 - 450 % | ASTM D638 |
| Tensile Modulus | 0.392 GPa | 56.9 ksi | ASTM D638 |
| Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
| Compressive Strength | 5.00 - 6.00 MPa @Temperature 25.0 °C |
725 - 870 psi @Temperature 77.0 °F |
1% deformation; ASTM D695 |
| Izod Impact, Unnotched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
| Coefficient of Friction | 0.020 - 0.038 | 0.020 - 0.038 | Non-lubricating |
| 0.020 - 0.0385 | 0.020 - 0.0385 | Lubricating | |
| Coefficient of Friction, Static | 0.020 | 0.020 | Coated-steel surface |
| Taber Abrasion, mg/1000 Cycles | <= 5.0 | <= 5.0 | Calculated using estimated density, 9.8 N load, cs-10 wheel |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 100 µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
| Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
| Melting Point | 327 °C | 621 °F | |
| Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous use |
| Flammability, UL94 | V-0 | V-0 | |
| Oxygen Index | >= 95 % | >= 95 % | ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
| Dielectric Constant | 2.1 @Frequency 1000 Hz |
2.1 @Frequency 1000 Hz |
ASTM D150 |
| 2.1 @Frequency 1e+6 Hz |
2.1 @Frequency 1e+6 Hz |
ASTM D150 | |
| Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
Short time; ASTM D149 |
| Dissipation Factor | <= 0.000010 @Frequency 1000 Hz |
<= 0.000010 @Frequency 1000 Hz |
ASTM D150 |
| 0.000020 @Frequency 1e+6 Hz |
0.000020 @Frequency 1e+6 Hz |
ASTM D150 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Chemical Resistance | Excellent | |
| Contact Angle | 110 | Angle to level |
| Weatherability | Excellent |