Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ASTM D792
Water Absorption 0.23 %
0.23 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.4 MPa
6000 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 64.1 MPa
9300 psi
ASTM D790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in