Ex-Tech Plastics VersaTech™ APET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Ex-Tech Plastics
Trade Name VersaTech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ex-Tech Plastics VersaTech™ APET.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ex-Tech VersaTech™ APET has exceptional properties such as visual transparency high heat distortion and it has good resistance to mineral oils, solvents and acids.Characteristics:TransparentExceptional visual propertiesSuperior performance in critical consumer applications End Uses:Food and medical traysConsumer packaging: clamshell, blister and trayInformation provided by Ex-Tech Plastics Inc.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
Viscosity Measurement >= 0.75
>= 0.75
Intrinsic Viscosity; ASTM D3835
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 250 %
250 %
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point >= 240 °C
>= 464 °F
Optical Properties Metric English Comments
Haze <= 2.0 %
<= 2.0 %
ASTM D1003
Transmission, Visible >= 90 %
>= 90 %
ASTM D1003
Descriptive Properties Value Comments
Clarity >99%
ASTM D1003