Overview of materials for Polyvinyl Dichloride (PVDC)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyvinyl Dichloride (PVDC).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.26 - 1.78 g/cc
0.0455 - 0.0643 lb/in³
Average value: 1.62 g/cc Grade Count:36
Filler Content 30.0 - 60.0 %
30.0 - 60.0 %
Average value: 50.0 % Grade Count:19
Water Absorption 0.130 - 1.80 %
0.130 - 1.80 %
Average value: 0.299 % Grade Count:13
pH 1.20 - 4.00
1.20 - 4.00
Average value: 2.28 Grade Count:5
Water Vapor Transmission 14.0 - 160 g/m²/day

@Temperature 38.0 - 38.0 °C
0.902 - 10.3 g/100 in²/day

@Temperature 100 - 100 °F
Average value: 50.7 g/m²/day Grade Count:5
11.0 - 160 g/m²/day

@Temperature 38.0 - 38.0 °C
0.708 - 10.3 g/100 in²/day

@Temperature 100 - 100 °F
Average value: 50.7 g/m²/day Grade Count:9
11.0 - 160 g/m²/day

@Thickness 0.00100 - 0.00100 mm
0.708 - 10.3 g/100 in²/day

@Thickness 0.0000394 - 0.0000394 in
Average value: 50.7 g/m²/day Grade Count:9
Oxygen Transmission 0.00400 - 0.0470 cc-mm/m²-24hr-atm
0.0102 - 0.119 cc-mil/100 in²-24hr-atm
Average value: 0.0219 cc-mm/m²-24hr-atm Grade Count:10
Oxygen Transmission Rate 40.0 - 1000 cc/m²/day
2.58 - 64.4 cc/100 in²/day
Average value: 292 cc/m²/day Grade Count:6
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00204 cm/cm Grade Count:12
Surface Tension 33.0 - 54.0 dynes/cm
33.0 - 54.0 dynes/cm
Average value: 41.6 dynes/cm Grade Count:5
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 14.0 - 280 MPa
2030 - 40600 psi
Average value: 237 MPa Grade Count:18
Elongation at Break 1.80 - 110 %
1.80 - 110 %
Average value: 8.79 % Grade Count:20
Modulus of Elasticity 1.03 - 24.0 GPa
149 - 3480 ksi
Average value: 18.3 GPa Grade Count:19
Flexural Yield Strength 240 - 400 MPa
34800 - 58000 psi
Average value: 350 MPa Grade Count:13
Flexural Modulus 11.5 - 23.5 GPa
1670 - 3410 ksi
Average value: 18.3 GPa Grade Count:13
Izod Impact, Notched 0.700 - 1.20 J/cm
1.31 - 2.25 ft-lb/in
Average value: 1.03 J/cm Grade Count:10
Izod Impact, Unnotched 4.60 - 11.0 J/cm
8.62 - 20.6 ft-lb/in
Average value: 7.98 J/cm Grade Count:10
Coefficient of Friction 0.210 - 0.350
0.210 - 0.350
Average value: 0.314 Grade Count:8
Thermal Properties Metric English Comments
CTE, linear 14.0 - 18.0 µm/m-°C
7.78 - 10.0 µin/in-°F
Average value: 15.6 µm/m-°C Grade Count:10
Deflection Temperature at 1.8 MPa (264 psi) 220 - 230 °C
428 - 446 °F
Average value: 228 °C Grade Count:12
Glass Transition Temp, Tg 7.00 - 16.0 °C
44.6 - 60.8 °F
Average value: 12.8 °C Grade Count:8
Flammability, UL94 HB - 5VA
HB - 5VA
Grade Count:8
Oxygen Index 25.0 - 37.0 %
25.0 - 37.0 %
Average value: 27.4 % Grade Count:8
Glow Wire Test 775 - 960 °C
1430 - 1760 °F
Average value: 866 °C Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Average value: 1.00e+13 ohm-cm Grade Count:5
Dielectric Constant 3.90 - 4.60
3.90 - 4.60
Average value: 4.33 Grade Count:7
Dielectric Strength 24.0 - 31.0 kV/mm
610 - 787 kV/in
Average value: 27.8 kV/mm Grade Count:6
Dissipation Factor 0.00900 - 0.0120
0.00900 - 0.0120
Average value: 0.0105 Grade Count:5
Comparative Tracking Index 400 - 600 V
400 - 600 V
Average value: 546 V Grade Count:6
Processing Properties Metric English Comments
Nozzle Temperature 260 - 290 °C
500 - 554 °F
Average value: 275 °C Grade Count:11
Melt Temperature 250 - 290 °C
482 - 554 °F
Average value: 269 °C Grade Count:19
Mold Temperature 120 - 140 °C
248 - 284 °F
Average value: 130 °C Grade Count:19
Drying Temperature 80.0 - 120 °C
176 - 248 °F
Average value: 114 °C Grade Count:19