Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | |
Plastcom SLOVAMID 6/66 FRc 3 TS PA6/66, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural colour. PA 6 + PA 66 alloy for injection moulding with increased flammability resistance, with nonhalogen flame retardant. Excellent.. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | STN EN ISO 294-4 |
Plastcom SLOVAMID® 6 GF 25 FRC 4 PA6 reinforced with glass fiber, flame retarded PA 6 for injection molding, reinforced with 25 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability according to UL 94 3 at 1,6mm, glow wire at 960°C. Applic.. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | STN EN ISO 294-4 |
Plastcom SLOVAMID® 6/66 FRC 3 TS PA6/66 flame retarded, heat stabilized PA 6 + PA 66 alloy for injection molding, reinforced with 30 % glass fiber, flame retarded with non halogen flame retardant, heat stabilized. Main features: flammability in accordance with UL 94 5 a.. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | ASTM D955 |
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | ASTM D955 |
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | ASTM D955 |
Oxford Polymers 604-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | ASTM D955 |
Oxford Polymers 802-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | ASTM D955 |
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.0075 - 0.010 cm/cm | 0.0075 - 0.010 in/in | ASTM D955 |
PTS PCA-30G00 Impact Modified Polycarbonate/PBT Alloy For Cold Temperature Impact.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | per ATM D955. Post shrinkage is 0.4% at 72hr 120ºC per ASTM D1299. |
Plenco 7300 Phenolic, Nodular, Injection Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file.. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | Isotropy |
Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 20% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistanceAvailable in: Asia Pacific and EuropeProduct Applications:.. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | Isotropy |
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr.. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | ASTM D955 |
Plenco 3597 Phenolic, Granular, Injection Molded PLENCO 03597 is a mineral filled phenolic molding compound offering excellent flammability ratings even at thin cross sections, along with excellent arc and comparative track resistance values. UL r.. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | Bayer Test |
Covestro Bayflex® 190 Polyurethane Elastomeric RIM, 20% Mica Filled, MDI-based 2-Component Liquid System 0.150 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | |
Cytec EN-2532 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | |
Cytec EN-2551 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Linear Mold Shrinkage | 0.0075 - 0.0085 cm/cm | 0.0075 - 0.0085 in/in | ASTM D955 |
Buckeye Polymers BP RPPC 1020 TU BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | ASTM D955 |
Adell AJ-13 Nylon 66, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | ASTM D955 |
Adell AJ-33 Nylon 66, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | ASTM D955 |
Adell BJ-33 Nylon 6, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | ASTM D955 |
Adell BT-33 Nylon 6, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0075 - 0.0083 cm/cm | 0.0075 - 0.0083 in/in | IS 13411-1992 |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | ASTM D955 |
Ashley Polymers Ashlene® P284 PPE Alloy, 10% Glass Reinforced A 10% glass reinforced PPE Alloy for superior properties and chemical resistance with high heat resistance.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | ASTM D955 |
Adell BJ-13 Nylon 6, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | restricted |
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry) Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi.. |
|||
Linear Mold Shrinkage | 0.0075 - 0.0090 cm/cm | 0.0075 - 0.0090 in/in | IS 13411-1992 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication .. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Conditioned) Ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | |
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |