Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Multibase Multi-Flex® TPE G 7680 NAT The burn rate is 1.2 in/min (30 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
RheTech Products FRP102-00 Polypropylene, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® ESD 5500 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5500 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5500 can be injectio.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | With Flow; ISO 2577 |
Polykemi AB SCANAMID 66 A53^EM Nylon 66, Modified Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.016 - 0.022 cm/cm | 0.016 - 0.022 in/in | ASTM D955 |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Linear Mold Shrinkage | 0.016 - 0.022 cm/cm | 0.016 - 0.022 in/in | ASTM D955 |
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Linear Mold Shrinkage | 0.016 - 0.022 cm/cm | 0.016 - 0.022 in/in | ASTM D955 |
Polymer Resources TP-GP2 Polybutylene Terephthalate, General Purpose Polybutylene Terephthalate, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | Flow |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.016 - 0.025 cm/cm | 0.016 - 0.025 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 ND Nylon 6 Nylon 6, low viscosity, permanently flexible, dry impact resistant (dowels).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D995 |
Huntsman IROGRAN® A 78 E 4588 Polyester-Based TPU-High Performance Grade High Hydrolysis resistance and good crystallinity. Suggested for injection molding.Information provided by Huntsman |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ISO 294-4 |
Aardvark Polymers AARTEL® 1000 Rotational Molding Resin Aartel 1000 is our premium grade of toughened impact modified acetal copolymer. Aartel 1000 is formulated with high impact properties combined with extended mechanical properties and elevated resist.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | 0.125inch wall |
Spartech PP5312 Mica Reinforced Homopolymer Information provided by Spartech |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Teknor Apex Chemlon® 267 Nylon 6, Impact Modified Notes: Chemlon® is a product offering flexural modulus, impact and elongation properties suitable for convoluted tubing and wire coating applications. Features: Copolymer; Good Flexibility; Good .. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Teknor Apex Monprene® MP 1049 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Teknor Apex Monprene® MP-1389E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | |
Tisan TISESTER® Flame Retardant (V0). Heat Stabilized Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | |
Tisan TISLAMID® 66 Impact Modified Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | |
Polyram RamSter PF329G4 PBT, 20% Glass Fiber, Flame Retardant 20% Glass fiber reinforced, halogen free flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | 4 inch disk; ASTM D955 |
DSM Biomedical Elasthane™ 75D Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Diamond Polymers NYLON 6615 Black, Super Tough Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | |
E-Polymers TEKAMID® TA210ST Super Tough PA66, DAM Super ToughnessInformation provided by E-Polymers Co. Ltd. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM Data; MD |
BASF Ultramid® 1310-11 NF2001 PA66 (Dry) Ultramid 1310-11 NF2001 is a controlled crystallization, fast cycling PA6/6 which provides extremely fast cycle times and improved productivity over Ultramid 1000. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Ashley Polymers Ashlene® 525 Nylon 66 High impact Nylon 66 with good stiffness for injection molding.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Ashley Polymers Ashlene® 527 Nylon 66 A very high impact, slightly lubricated, nylon resin.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | Asahi Kasei Method |
Asahi Kasei Tenac®-C HC450 Copolymer Acetal Resin New Copolymer, the improvement of physical properties of standard gradesInformation provided by Asahi Kasei Corporation. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Aaron Industries AAROPRENE® AEN 6600-3 Nylon 6/6 Engineered Resin |
|||
Linear Mold Shrinkage | 0.016 - 0.022 cm/cm | 0.016 - 0.022 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PA 1408 Conductive Thermoplastic Compound PRE-ELEC® PA 1408 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |