Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 500 - 710 µm | 500 - 710 µm | |
Potters Industries A-Series P-0280 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 500 µm | 500 µm | ASTM D4895 |
3M Dyneon™ TFX 2035 PTFE
(discontinued **) Typical Applications: Liners, extruded tape, thick wall tubing.Information provided by the Dyneon division of 3M. |
|||
Particle Size | 500 µm | 500 µm | ASTM D4895 |
3M Dyneon™ TFM™ 2001 Modified PTFE Paste Extrusion Powder
(discontinued **) Type I, gr. 2 PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1000. Average particle size 500µm.Modified PTFE fine powder product for paste extrusion applications. The modified .. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 12086 |
3M Dyneon™ TFM™ 2001 PTFE
(discontinued **) Processable by standard paste extrusion methodRecommended for high performance applications with reduction ratios up to 1000:1Provides denser polymer structure with fewer micro voids and lower gas p.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5050 500 Micron LDPE Powder Description: ICOFLO 510-5050 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5053 500 Micron LDPE Powder Description: ICOFLO 510-5053 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5059 500 Micron LDPE Powder Description: ICOFLO 510-5059 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5062 500 Micron LDPE Powder Description: ICOFLO 510-5062 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOTEXâ„¢ 520-5056 500 Micron LDPE Powder Description: ICOTEX 520-5056 is a low density polyethylene powder that has been developed to meet the special requirement of the textile coating industry. Key Characteristics: very high flow, very g.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET 150 Dry Air-Setting Refractory Mortar Description: Adhesiet 150 is an air setting mortar with a sodium silicate bond and is supplied as a dry powder. Because of the special mix of the raw materials it can be used up to 1500°C.Remarks.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET 160 Dry Air-Setting Refractory Mortar Description: Adhesiet 160 is an air setting bauxite based mortar with a sodium silicate bond and it is supplied as a dry powder it can be used up to 1600°C.Remarks: The results of the chemical an.. |
|||
Particle Size | 500 µm | 500 µm | Finer than |
Inhance Fluoro-Seal INHANCE® UH-1080 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Particle Size | 500 - 5000 µm | 500 - 5000 µm | |
Minelco Chilcon Low grade FeSi Hard, wear resistant. Applications: Heavy aggregates, hard wearing floors |
|||
Particle Size | 500 µm | 500 µm | ASTM D 1921 |
Lucobit Lucofin® 1400MN Powder Ethylene Butyl Acrylate Lucofin 1400MN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN Powder is softer and more flexible ethane et.. |
|||
Particle Size | 500 - 700 µm | 500 - 700 µm | |
Shandong Dongyue Polymer DF-31B PTFE Pelletized Resin Usage: The resin is used to auto press molding and ram extrusion all kinds of rods, pipe etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF.. |
|||
Particle Size | 500 µm | 500 µm | |
Sterigenics Raprex® R-400A Thermoplastic Powder Applications: Extrusion CoatingsA thermoplastic powder based on polyethylene was developed by Sterigenics Advanced Applications for extrusion coating on metal and other surfaces. RAPREX™ 400 is.. |
|||
Particle Size | 500 - 2000 µm | 500 - 2000 µm | >90 |
Solvay Chemicals Ixper® 70C Calcium Peroxide IXPER® 70C Calcium Peroxide Granules are based on our commercial grade IXPER® 75C.EINECS Number: 215-139-4/CAS Number: 1305-79-9Information provided by Solvay |
|||
Particle Size | >= 500 µm | >= 500 µm | d90, 22%, Vibrated sieving |
TIMCAL TIMREX® KS150-600SP Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 500 µm | 500 µm | |
Daikin POLYFLON F-302 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Small to large diameter tubes, flexible hoses, shrinkable tubes, heavy duty electric wires smaller than AGW18, and jackets.Information provided by .. |
|||
Particle Size | 500 µm | 500 µm | ASTM D4894 |
Daikin POLYFLON M-393 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding, automatic compression molding, and ram extrusion.Features: Maximum emphasis given to ease of handling during molding. Used when molded arti.. |
|||
Particle Size | >= 500 µm | >= 500 µm | 0.03 |
Arkema Group OREVAC® 18345 RNP Pipe Coating Binder Resin OREVAC 18345 RNP is a range of modified polyethylene which, when molten, have excellent adhesive properties to various substrates and are designed to bond dissimilar materials. It is supplied in bla.. |
|||
Particle Size | 500 - 850 µm | 500 - 850 µm | min 92%; BC HSZ 326:2001/1 screening |
BorsodChem ONGROSTYR F-I Expandable Polystyrene (EPS) ONGROSTYR F-I is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e... |
|||
Particle Size | 500 - 600 µm | 500 - 600 µm | |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
Particle Size | 500 µm | 500 µm | average; ISO 13320 |
3M Dyneon™ TF 2025Z PTFE Fine Powder Dyneon™ TF 2025 Z PTFE is an ideal grade for pipe liner applications in chemical plant construction due to high green strength.Product Features:High molecular weightFine powder grade for low to med.. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 12086 |
3M Dyneon™ TF 2029Z PTFE Fine Powder Dyneon™ TF 2029 Z PTFE is an ideal grade for tapes with high mechanical strength, such as electrical tape for wrapped insulations or flat cables. Also ideal for yarn applications, including sewing .. |
|||
Particle Size | 500 µm | 500 µm | VW-10300P; D90 Particle sizes by sieve measurement |
Solvay Specialty Polymers Virantage® VW-10300 P, FP Polyethersulfone (PESU)
(Unverified Data**) Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Two grades are offered: Virantage VW-10300P and Virantage VW-10300FP, providing two par.. |
|||
Particle Size | 500 µm | 500 µm | VW-10700RP; D90 Particle sizes by sieve measurement |
Solvay Specialty Polymers Virantage® VW-10700 RP, RFP, RSFP Polyethersulfone (PESU)
(Unverified Data**)&l Virantage® VW-series functionalized polyethersulfones (r-PESU) are amorphous, high-temperature sulfone polymers featuring reactive end groups to enhance solubility and improve interfacial propertie.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET 170 P Dry Air-Setting Refractory Mortar Description: Adhesiet 170 P is a phosphate bonded air setting mortar, supplied as a dry powder. Because of the special choice of raw materials this mortar is especially applied in aluminum melting a.. |