Material Notes:
Description: ICOTEX 520-5056 is a low density polyethylene powder that has been developed to meet the special requirement of the textile coating industry. Key Characteristics: very high flow, very good flexibility and excellent gloss. Information provided by ICO Polymers.A Schulman acquired ICO, Inc. in 2010.
Physical Properties Metric English Comments
Density 0.913 g/cc
0.0330 lb/in³
ASTM D1505
Particle Size >= 150 µm
>= 150 µm
pan, 9%
<= 500 µm
<= 500 µm
sieve < 5%
Melt Index of Compound 70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 8.00 MPa
1160 psi
ASTM D638
Tensile Strength, Yield 8.00 MPa
1160 psi
50 mm/min; ASTM D638
Elongation at Break 100 %
100 %
50 mm/min; ASTM D638
Thermal Properties Metric English Comments
Melting Point 100 °C
212 °F
DSC; ASTM D3418
130 °C
266 °F
fusing temperature
Vicat Softening Point 75.0 °C
167 °F
ASTM D1525
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D638
Descriptive Properties Value Comments
Max Dry Flow max 37 sec/100g
ASTM