Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ICO Polymers ICOFLOâ„¢ 510-5059 500 Micron LDPE Powder

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Masterbatch Grade
Manufacturer ICO Polymers (A Schulman Inc.)
Trade Name ICOFLO™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ICO Polymers ICOFLOâ„¢ 510-5059 500 Micron LDPE Powder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: ICOFLO 510-5059 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in masterbatch (instead of pellet), superior color development or additive dispersion can be achieved in the final concentrate. Key Characteristics: excellent heat stability. Information provided by ICO Polymers.A Schulman acquired ICO, Inc. in 2010.
Physical Properties Metric English Comments
Density 0.915 g/cc
0.0331 lb/in³
ASTM D1505
Particle Size >= 150 µm
>= 150 µm
pan, 13%
<= 500 µm
<= 500 µm
sieve < 5%
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 104 °C
219 °F
DSC; ASTM D3418
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Descriptive Properties Value Comments
Max Dry Flow max 31 sec/100g
ASTM
Users viewing this material also viewed the following: