Solvay Chemicals Ixper® 70C Calcium Peroxide

Category Ceramic , Oxide
Manufacturer Solvay Chemicals
Trade Name Ixper®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Ixper® 70C Calcium Peroxide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
IXPER® 70C Calcium Peroxide Granules are based on our commercial grade IXPER® 75C.EINECS Number: 215-139-4/CAS Number: 1305-79-9Information provided by Solvay
Physical Properties Metric English Comments
Bulk Density 0.860 - 0.960 g/cc
0.0311 - 0.0347 lb/in³
Particle Size 500 - 2000 µm
500 - 2000 µm
>90
pH 11.3 - 12.1
11.3 - 12.1
Molecular Weight 72.1 g/mol
72.1 g/mol
Descriptive Properties Value Comments
Appearance White yellowish, odor-less granules
Composition >15.5%
Available Oxygen
>70%
CaO2
15.76-16.64%
Available Oxygen, Typical Value
71-75%
CaO2, Typical Value