Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.07 - 1.51 g/cc | 0.0387 - 0.0546 lb/in³ | Average value: 1.30 g/cc Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Density | 1.38 - 1.51 g/cc | 0.0499 - 0.0546 lb/in³ | Average value: 1.44 g/cc Grade Count:10 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
Density | 1.16 - 1.51 g/cc | 0.0419 - 0.0546 lb/in³ | Average value: 1.38 g/cc Grade Count:16 |
Overview of materials for Nylon 66, Mineral Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v.. |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 612 Rigid PVC, Extrusion Spiral pipes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1184 |
Fainplast Compounds RK 0758 Rigid PVC, Extrusion Lead Free Electric corrugated pipes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1184 |
Fainplast Compounds RK 115 Rigid PVC, Extrusion Lead Free Small tubes for shoes |
|||
Density | 1.39 - 1.51 g/cc | 0.0502 - 0.0546 lb/in³ | Apparent |
Gouda Vuurvast FI 45-15 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1183 |
Fainplast Compounds AP 88 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 85 Flexible PVC, Sheathing Lead Free General purposes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 75/1 Flexible PVC, Sheathing General purposes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1183 |
Fainplast Compounds FK 86 Flexible PVC, Insulation Lead Free General purposes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 90/2 Flexible PVC, Insulation General purposes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 95 Flexible PVC, Insulation Power cables |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 70 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 83 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 85/UV Flexible PVC, Flame Retardant Sheathing Lead Free Sheathing low temperatures |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 039/1 Halogen Free PVC Sheathing, high flexibility |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 3621 Halogen Free PVC General purpose |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 411 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:SheathingInformation provided by Fainplast Compounds |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HFX 509 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Insulation for solar cablesInformation provided by Fainpla.. |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1183 |
Fainplast Compounds PMS 78 Flexible PVC, Extrusion Gas pipes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1183 |
Fainplast Compounds PMS 82 Flexible PVC, Extrusion Gas pipes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 116 Rigid PVC, Extrusion Small tubes for shoes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 010 Flexible PVC, Sheathing Lead Free General purposes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 211 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Insulation and sheathing, improved processabilityInformation provided by Fainplast Compo.. |
|||
Density | 0.950 - 1.51 g/cc | 0.0343 - 0.0546 lb/in³ | Average value: 1.20 g/cc Grade Count:482 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 213 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:General purpose, improved processabilityInformation provided by Fainplast Compounds |
|||
Density | 1.15 - 1.51 g/cc | 0.0415 - 0.0546 lb/in³ | Average value: 1.32 g/cc Grade Count:28 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |
|||
Density | 1.00 - 1.51 g/cc | 0.0361 - 0.0546 lb/in³ | Average value: 1.14 g/cc Grade Count:288 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |
|||
Density | 1.12 - 1.51 g/cc @Temperature 250 - 260 °C |
0.0405 - 0.0546 lb/in³ @Temperature 482 - 500 °F |
Average value: 1.27 g/cc Grade Count:6 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |