| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.47 g/cc | 0.0531 lb/in³ | |
|
Plastcom SLOVAMID 6 GF 30 FRA 3 PA6, 30% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 850°C,..
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP KONDUIT PX10322 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compound, with through-plane and in-plane thermal conductivity of 1.7 W/(m*K) and 4.7 W/(m*K) respectively, conforming to ASTM E 1461 test standard.
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM Data |
|
Dow Questra® EA514 High Heat Syndiotactic Polystyrene, 40% Glass Filled
(discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
|
|||
| Density | 1.47 - 1.61 g/cc | 0.0531 - 0.0582 lb/in³ | Average value: 1.52 g/cc Grade Count:12 |
|
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and ..
|
|||
| Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1184 |
|
Fainplast Compounds RK 0758 Rigid PVC, Extrusion Lead Free
Electric corrugated pipes
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
Solvay Specialty Polymers Amodel® A-8930 HS Polyphthalamide (PPA), 30% Glass Fiber
Amodel® A-8930 HS is a 30% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low..
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly (Asia Pacific)
LNP* Stat-kon* KE004 is a compound based on Acetal Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® PA6/6 GF/M40 ML2 GY 40% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and He..
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK
LNP* THERMOCOMP* LC008E is a compound based on Polyetheretherketone resin containing 40% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF008H PA 66
LNP* THERMOCOMP* RF008H is a compound based on Nylon 66 containing 40% Glass Fiber. Added feature of this grade is: Healthcare.
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183/A |
|
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, Conditioned
Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15..
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
Teijin Panlite® GV-3430R High Flame Retardancy, Glass Fiber Reinforced Polycarbonate Resin
GF 30% reinforced, improved flame retardance and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecis..
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
|
Plenco 4485 Phenolic, Granular, Compression Molded
PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a..
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
Wellman Wellamid® MR410 42H-N 40% Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
Unitika TERRAMAC TE-7300 Polylactic Acid (PLA)
Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
Polyplastics FR-PET® B3015FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 6, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
CP-Polymer-Technik Wellamid® 6000 MX 400 CP Combination Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
EMS-Grivory Grivory® LVX-50H nat PA12-GF50
Product description: Grilamid LVX-50H natural is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and st..
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
Eurotec® Tecodur® PB70 GR20 NL CA 01 PBT/PET 20% glass fiber reinforced
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
|
Adell AH-38 Nylon 66, 40% Mineral Filled
Data provided by Adell Plastics, Inc.
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM
Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite..
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
BASF Ultradur S 4090 G6 30% Glass Filled PBT
Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati..
|
|||
| Density | 1.47 - 1.87 g/cc | 0.0531 - 0.0676 lb/in³ | Average value: 1.68 g/cc Grade Count:22 |
|
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
|
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 30% of glass fibers for industrial parts with high dimensional stab..
|
|||
| Density | 1.47 g/cc | 0.0531 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
|
Arlon 43362X0055 0.0055" (0.140 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2112 FiberglassFlame Resistance: Product meets Title 14 CFR 25.856(a) Appendix F, Part VI (amdt. 25-111) fl..
|
|||