Gouda Vuurvast FI 45-15 Insulating Refractory Brick

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Gouda Vuurvast FI 45-15 Insulating Refractory Brick.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 1.39 - 1.51 g/cc
0.0502 - 0.0546 lb/in³
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 12.0 - 18.0 MPa
1740 - 2610 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.500 - 0.700 W/m-K

@Temperature 200 °C
3.47 - 4.86 BTU-in/hr-ft²-°F

@Temperature 392 °F
0.530 - 0.730 W/m-K

@Temperature 600 °C
3.68 - 5.07 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.600 - 0.800 W/m-K

@Temperature 1000 °C
4.16 - 5.55 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1450 °C
2640 °F
Shrinkage -0.600 - -0.200 %

@Temperature 1420 °C,
Time 86400 sec
-0.600 - -0.200 %

@Temperature 2590 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 47 %
47 %
Fe2O3 <= 1.5 %
<= 1.5 %
SiO2 47 %
47 %
Descriptive Properties Value Comments
Segercone 35