Overview of materials for Thermoplastic Polyimide, Carbon Fiber

Category Polymer , Thermoplastic , Polyimide, Thermoplastic , Thermoplastic Polyimide, Carbon Fiber
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Thermoplastic Polyimide, Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.38 - 1.51 g/cc
0.0499 - 0.0546 lb/in³
Average value: 1.44 g/cc Grade Count:10
Filler Content 20.0 - 30.0 %
20.0 - 30.0 %
Average value: 26.7 % Grade Count:3
Water Absorption 0.100 - 0.690 %
0.100 - 0.690 %
Average value: 0.257 % Grade Count:4
0.660 - 4.17 %

@Temperature 80.0 - 80.0 °C
0.660 - 4.17 %

@Temperature 176 - 176 °F
Average value: 2.33 % Grade Count:2
2.24 - 2.24 %

@Temperature 80.0 - 80.0 °C
2.24 - 2.24 %

@Temperature 176 - 176 °F
Average value: 2.33 % Grade Count:1
2.24 - 2.24 %

@Time 86400 - 86400 sec
2.24 - 2.24 %

@Time 24.0 - 24.0 hour
Average value: 2.33 % Grade Count:1
Linear Mold Shrinkage 0.000100 - 0.00400 cm/cm
0.000100 - 0.00400 in/in
Average value: 0.00183 cm/cm Grade Count:6
Mechanical Properties Metric English Comments
Hardness, Shore D 89.0 - 91.0
89.0 - 91.0
Average value: 90.0 Grade Count:3
Tensile Strength, Ultimate 36.5 - 241 MPa
5300 - 35000 psi
Average value: 174 MPa Grade Count:7
Elongation at Break 0.800 - 5.50 %
0.800 - 5.50 %
Average value: 2.17 % Grade Count:6
Elongation at Yield 1.80 - 4.30 %
1.80 - 4.30 %
Average value: 2.67 % Grade Count:5
Modulus of Elasticity 4.50 - 29.0 GPa
653 - 4200 ksi
Average value: 16.5 GPa Grade Count:8
Flexural Yield Strength 97.9 - 345 MPa
14200 - 50000 psi
Average value: 225 MPa Grade Count:10
Flexural Modulus 4.24 - 25.5 GPa
615 - 3700 ksi
Average value: 12.6 GPa Grade Count:10
Compressive Yield Strength 184 - 474 MPa
26700 - 68700 psi
Average value: 279 MPa Grade Count:4
Izod Impact, Notched 0.801 - 1.07 J/cm
1.50 - 2.00 ft-lb/in
Average value: 0.921 J/cm Grade Count:4
Izod Impact, Unnotched 4.81 - 6.41 J/cm
9.00 - 12.0 ft-lb/in
Average value: 5.94 J/cm Grade Count:4
Charpy Impact Unnotched 1.96 - 3.74 J/cm²
9.33 - 17.8 ft-lb/in²
Average value: 2.90 J/cm² Grade Count:3
3.50 - 3.50 J/cm²

@Temperature -30.0 - -30.0 °C
16.7 - 16.7 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.50 J/cm² Grade Count:1
Charpy Impact, Notched 1.00 - 1.00 J/cm²

@Temperature -30.0 - -30.0 °C
4.76 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.00 J/cm² Grade Count:1
Compression Set 49.0 - 98.0 %
49.0 - 98.0 %
Average value: 69.0 % Grade Count:3
Thermal Properties Metric English Comments
CTE, linear 41.0 - 88.0 µm/m-°C

@Temperature 50.0 - 300 °C
22.8 - 48.9 µin/in-°F

@Temperature 122 - 572 °F
Average value: 61.0 µm/m-°C Grade Count:3
CTE, linear, Transverse to Flow 43.0 - 67.0 µm/m-°C

@Temperature 50.0 - 300 °C
23.9 - 37.2 µin/in-°F

@Temperature 122 - 572 °F
Average value: 54.5 µm/m-°C Grade Count:2
Deflection Temperature at 1.8 MPa (264 psi) 240 - 340 °C
464 - 644 °F
Average value: 297 °C Grade Count:5
Flammability, UL94 V-0
V-0
Grade Count:7
Electrical Properties Metric English Comments
Surface Resistance 10000 - 1.00e+12 ohm
10000 - 1.00e+12 ohm
Average value: 1.40e+11 ohm Grade Count:4
Processing Properties Metric English Comments
Processing Temperature 371 - 410 °C
700 - 770 °F
Average value: 384 °C Grade Count:3
Melt Temperature 370 - 416 °C
698 - 780 °F
Average value: 392 °C Grade Count:5
Mold Temperature 177 - 232 °C
350 - 450 °F
Average value: 200 °C Grade Count:6
Drying Temperature 180 - 204 °C
356 - 400 °F
Average value: 196 °C Grade Count:5
Moisture Content 0.0100 %
0.0100 %
Average value: 0.0100 % Grade Count:3
Dew Point -40.0 °C
-40.0 °F
Average value: -40.0 °C Grade Count:3
Injection Pressure 138 - 193 MPa
20000 - 28000 psi
Average value: 165 MPa Grade Count:4