Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Orbilan RubberLen® R55 HMW-PE, dark blue ORBILAN RUBBERLEN® is a two-layered laminated panel made from Thermoplastic Elastomer (TPE) and low-pressure Polyethylene of High Molecular Weight (HMW-PE). RUBBERLEN® distinguishes itself by very.. |
|||
Density | 0.950 - 0.954 g/cc | 0.0343 - 0.0345 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4152L (524F6) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.949 - 0.953 g/cc | 0.0343 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6752E (516H5) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® HE-Y449-A HDPE Extrusion Resin Features: High ESCR, good toughness, good chemical resistance, good processability.Applications: Pipe coatings, profile extrusions, sheet extrusion for thermoforming, corrugated tubing, conduit.Data.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Advanced Elastomer Systems VistaFlex® 912-B Thermoplastic Rubber
(discontinued **) Description: A black super high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM Data |
Americas Styrenics Styron® 6187SF High Impact Polystyrene
(discontinued **) STYRON® 6187SF structural foam molding resin is a high impact polystyrene grade with proprietary ignition resistance additive package to achieve UL 94 V-0 rating. It offers excellent moldability an.. |
|||
Density | 0.950 - 0.954 g/cc | 0.0343 - 0.0345 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4153L (524F6) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Total Evatane® 28 - 03 HDPE, blown film
(discontinued **) EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 130 to 160.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Total Lacqtene® 2003 PBK 41 HDPE pipe, sheet
(discontinued **) LACQTENE® 2003 PBK 41 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2003 PBK 41 is a black compound especially developed for i.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | Exxon Method |
ExxonMobil Escorene® UL-7740 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Manifattura Cattaneo PE HD Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | Not Compounded |
KKPC KOSYN 1712 Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D4883 |
Ineos G50-100 HDPE Ineos G50-100 is a high molecular weight, high density polyethylene copolymer developed for sheet extrusion, thermoforming and large part blowmolding where the finished product demands outstanding p.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | |
JPJ Technologies 2300XM HDPE Extrusion Information provided by JPJ Technologies |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L5005V High Density Polyethylene, HMW Film Grade ALATHON L5005V is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typical applicati.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ISO 1183 |
Borealis Borstar® ME3446 Yellow Polyethylene Compound for The Coextrusion of Identifying Stripes On Black MD Pipe for Natural Gas Borstar 3446 is a bimodal, cadmium free, medium density polyethylene compound designed for coextrusion of yellow identifying stripes. It is fully stabilized against thermal degradation and the die .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® BB 29 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
DuPont Conpol™ 10AF Ethylene-Methacrylic Acid Additive Resin Conpol™ additive resins, supplied in pellet form, are designed to modify the surface properties of films or coatings of Surlyn® ionomer resins and Nucrel® acid copolymer resins. They are concentr.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Total 1285 HDPE film Applications: T-shirt sacks, trash can liners, merchandise bags, coex applicationsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
DuPont Bynel® 3861 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® E924ND Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E924ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D4883 |
ExxonMobil Paxon™ BA50-100 Blow Molding Resin Product Description: BA50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: .. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HHM 4903 High Density Ethylene Hexene Copolymer High Density Ethylene Hexene CopolymerCustomer Benefits: A high performance copolymer that can measure up to the most demanding application. Specifically formulated to provide toughness and durabil.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Copolymer CP0437M10CL Mica Reinforced Coupled |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Teknor Apex Sarlink® 4139D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4139D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Orbilan RubberLen® 70 HMW-PE, dark blue ORBILAN RUBBERLEN® is a two-layered laminated panel made from Thermoplastic Elastomer (TPE) and low-pressure Polyethylene of High Molecular Weight (HMW-PE). RUBBERLEN® distinguishes itself by very.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ISO 1183 |
Total XT10 N Natural HDPE, pipe Applications: Potable water, industrial and mining, sewer and sewer relining, gas and oil gathering, general pipe relining, pipe coatingInformation provided provided by Total Petrochemicals.Total Pe.. |
|||
Density | 0.950 g/cc @Temperature 25.0 °C |
0.0343 lb/in³ @Temperature 77.0 °F |
Liquid |
Solvay Specialty Polymers Meforex® 143a Ozone-Friendly CFC Replacement Formula: CH3CF3; Name: 1,1,1 Trifluoroethane. Replaces R 502. Refrigerant blends components for low and middle temperatures.Information provided by Solvay Solexis, Inc. |