Physical Properties Metric English Comments
Density 1.50 - 1.60 g/cc
0.0542 - 0.0578 lb/in³
Prodways PLASTCure Rigid 10 500 3D Printing Polymer
Superior thermo-mechanical properties.Suitable for the manufacture of parts that require thermal stability, extreme accuracy and quick turnaround. Exceptional for parts that are designed for wind tu..
Density 1.47 - 1.60 g/cc

@Temperature 250 - 260 °C
0.0531 - 0.0578 lb/in³

@Temperature 482 - 500 °F
Average value: 1.54 g/cc Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Density 1.36 - 1.60 g/cc
0.0491 - 0.0578 lb/in³
Average value: 1.44 g/cc Grade Count:13
Overview of materials for PEKK, Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M..
Density 1.10 - 1.60 g/cc
0.0397 - 0.0578 lb/in³
Average value: 1.24 g/cc Grade Count:254
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
Density 1.59 - 1.60 g/cc
0.0574 - 0.0578 lb/in³
Average value: 1.59 g/cc Grade Count:5
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E..
Density 1.45 - 1.60 g/cc
0.0524 - 0.0578 lb/in³
Average value: 1.53 g/cc Grade Count:21
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum ..
Density 1.34 - 1.60 g/cc
0.0484 - 0.0578 lb/in³
Average value: 1.51 g/cc Grade Count:3
Overview of materials for Phenolic/Rubber; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp..
Density 1.48 - 1.60 g/cc
0.0535 - 0.0578 lb/in³
Average value: 1.52 g/cc Grade Count:12
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Density 1.14 - 1.60 g/cc
0.0412 - 0.0578 lb/in³
Average value: 1.28 g/cc Grade Count:250
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Density 1.12 - 1.60 g/cc
0.0405 - 0.0578 lb/in³
Average value: 1.29 g/cc Grade Count:122
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Density 1.10 - 1.60 g/cc
0.0397 - 0.0578 lb/in³
Average value: 1.33 g/cc Grade Count:12
Overview of materials for Nylon 66, 10% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ..
Density 1.45 - 1.60 g/cc
0.0524 - 0.0578 lb/in³
Compounded
Epichlorohydrin Rubber (CO, ECO)
CO is the ISO designation for the homopolymer and ECO is the ISO designation for the ethylene oxide copolymer. Epichlorohydrin rubber is generally damaged by chlorinated solvents, ketones, aldehyde..
Density 1.45 - 1.60 g/cc
0.0524 - 0.0578 lb/in³
Compounded
Chlorosulfonated Polyethylene Rubber (CM, CSM)
The chlorine (in CM) or chlorine and chlorosulfonyl (CSM) groups prevent the crystallization that occurs on unmodified polyethylene.
Density 1.56 - 1.60 g/cc
0.0564 - 0.0578 lb/in³
ISO R 1184
Fainplast Compounds RE 330 Rigid PVC, Extrusion
Various profiles
Density 1.56 - 1.60 g/cc
0.0564 - 0.0578 lb/in³
ISO R 1184
Fainplast Compounds RE 425 Rigid PVC, Extrusion
Electric channels
Density 1.56 - 1.60 g/cc
0.0564 - 0.0578 lb/in³
ISO R 1184
Fainplast Compounds RE 425/R Rigid PVC, Extrusion
Shiny electric channels
Density 1.56 - 1.60 g/cc
0.0564 - 0.0578 lb/in³
ISO R 1184
Fainplast Compounds RH 306/W Rigid PVC, Antishock Extrusion
Antishock profiles
Density 1.56 - 1.60 g/cc
0.0564 - 0.0578 lb/in³
ISO R 1184
Fainplast Compounds RK 335/1 Rigid PVC, Extrusion Lead Free
Profiles
Density 1.50 - 1.60 g/cc
0.0542 - 0.0578 lb/in³
Chengdu Polyster MCA Melamine Cyanurate
White crystal power with satiny. It is an excellent non-halogen N flame retardant. The product is mainly used as non-halogen flame retardant for synthetic resin(PA, PVC, PS, POM), synthetic rubber a..
Density 1.45 - 1.60 g/cc
0.0524 - 0.0578 lb/in³
Molding; IS 867-1963
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded
Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg..
Density 1.11 - 1.60 g/cc
0.0401 - 0.0578 lb/in³
Average value: 1.30 g/cc Grade Count:112
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Density 1.46 - 1.60 g/cc
0.0527 - 0.0578 lb/in³
Average value: 1.51 g/cc Grade Count:9
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..