Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.10 - 1.60 g/cc
0.0397 - 0.0578 lb/in³
Average value: 1.24 g/cc Grade Count:254
1.02 - 1.03 g/cc
<br>@Temperature 260 - 260 °C
0.0368 - 0.0372 lb/in³
<br>@Temperature 500 - 500 °F
Average value: 1.02 g/cc Grade Count:15
Water Absorption 0.0300 - 0.500 %
0.0300 - 0.500 %
Average value: 0.215 % Grade Count:55
Moisture Absorption at Equilibrium 0.0300 - 0.200 %
0.0300 - 0.200 %
Average value: 0.122 % Grade Count:102
Water Absorption at Saturation 0.0100 - 0.500 %
0.0100 - 0.500 %
Average value: 0.339 % Grade Count:85
Viscosity 100000 - 295000 cP
100000 - 295000 cP
Average value: 233000 cP Grade Count:12
Maximum Moisture Content 0.0200
0.0200
Average value: 0.0200 Grade Count:17
Linear Mold Shrinkage 0.0000300 - 0.0200 cm/cm
0.0000300 - 0.0200 in/in
Average value: 0.00889 cm/cm Grade Count:211
Linear Mold Shrinkage, Transverse 0.00110 - 0.0180 cm/cm
0.00110 - 0.0180 in/in
Average value: 0.00975 cm/cm Grade Count:44
Melt Flow 1.90 - 60.0 g/10 min
1.90 - 60.0 g/10 min
Average value: 14.5 g/10 min Grade Count:169
Mechanical Properties Metric English Comments
Hardness, Rockwell L 80.0 - 89.0
80.0 - 89.0
Average value: 86.8 Grade Count:4
Hardness, Rockwell R 95.0 - 119
95.0 - 119
Average value: 113 Grade Count:25
Hardness, H358/30 81.0 - 114 MPa
11700 - 16500 psi
Average value: 97.2 MPa Grade Count:29
Hardness, Shore D 76.0 - 79.0
76.0 - 79.0
Average value: 76.6 Grade Count:5
Tensile Strength, Ultimate 30.0 - 110 MPa
4350 - 16000 psi
Average value: 49.7 MPa Grade Count:131
20.0 - 20.0 MPa
<br>@Temperature 60.0 - 60.0 °C
2900 - 2900 psi
<br>@Temperature 140 - 140 °F
Average value: 20.0 MPa Grade Count:1
Tensile Strength, Yield 33.0 - 122 MPa
4790 - 17700 psi
Average value: 53.4 MPa Grade Count:223
Elongation at Break 2.00 - 250 %
2.00 - 250 %
Average value: 97.2 % Grade Count:216
75.0 - 75.0 %
<br>@Temperature 60.0 - 120 °C
75.0 - 75.0 %
<br>@Temperature 140 - 248 °F
Average value: 91.7 % Grade Count:1
Elongation at Yield 2.00 - 20.0 %
2.00 - 20.0 %
Average value: 4.57 % Grade Count:136
>= 10.0 %
<br>@Temperature 60.0 - 120 °C
>= 10.0 %
<br>@Temperature 140 - 248 °F
Average value: 10.0 % Grade Count:1
Modulus of Elasticity 1.40 - 5.12 GPa
203 - 743 ksi
Average value: 2.33 GPa Grade Count:141
1.00 - 1.40 GPa
<br>@Temperature 60.0 - 120 °C
145 - 203 ksi
<br>@Temperature 140 - 248 °F
Average value: 1.20 GPa Grade Count:1
Flexural Yield Strength 43.0 - 183 MPa
6240 - 26500 psi
Average value: 82.0 MPa Grade Count:210
Flexural Modulus 1.55 - 19.3 GPa
225 - 2800 ksi
Average value: 2.35 GPa Grade Count:214
Izod Impact, Notched 0.350 - 981 J/cm
0.656 - 1840 ft-lb/in
Average value: 7.00 J/cm Grade Count:191
0.300 - 7.50 J/cm
<br>@Temperature -50.0 - 0.000 °C
0.562 - 14.1 ft-lb/in
<br>@Temperature -58.0 - 32.0 °F
Average value: 3.76 J/cm Grade Count:89
1.00 - 7.84532 J/cm
<br>@Temperature -40.0 - -20.0 °C
1.87 - 14.6975 ft-lb/in
<br>@Temperature -40.0 - -4.00 °F
Average value: 3.76 J/cm Grade Count:35
1.00 - 7.84532 J/cm
<br>@Thickness 1.57 - 6.40 mm
1.87 - 14.6975 ft-lb/in
<br>@Thickness 0.0618 - 0.252 in
Average value: 3.76 J/cm Grade Count:35
Izod Impact, Unnotched 4.30 J/cm - NB
8.06 ft-lb/in - NB
Average value: 14.8 J/cm Grade Count:29
3.20 J/cm - NB
<br>@Temperature -30.0 - -30.0 °C
5.99 ft-lb/in - NB
<br>@Temperature -22.0 - -22.0 °F
Average value: 4.07 J/cm Grade Count:13
4.50 - 4.50 J/cm
<br>@Temperature -40.0 - -40.0 °C
8.43 - 8.43 ft-lb/in
<br>@Temperature -40.0 - -40.0 °F
Average value: 4.07 J/cm Grade Count:1
4.50 - 4.50 J/cm
<br>@Thickness 3.20 - 3.20 mm
8.43 - 8.43 ft-lb/in
<br>@Thickness 0.126 - 0.126 in
Average value: 4.07 J/cm Grade Count:1
Izod Impact, Notched (ISO) 4.00 - 65.0 kJ/m²
1.90 - 30.9 ft-lb/in²
Average value: 45.1 kJ/m² Grade Count:95
3.00 - 65.0 kJ/m²
<br>@Temperature -40.0 - 0.000 °C
1.43 - 30.9 ft-lb/in²
<br>@Temperature -40.0 - 32.0 °F
Average value: 27.3 kJ/m² Grade Count:100
Izod Impact, Unnotched (ISO) 31.0 kJ/m² - NB
14.8 ft-lb/in² - NB
Average value: 32.7 kJ/m² Grade Count:30
20.0 kJ/m² - NB
<br>@Temperature -40.0 - -30.0 °C
9.52 ft-lb/in² - NB
<br>@Temperature -40.0 - -22.0 °F
Average value: 20.0 kJ/m² Grade Count:34
Charpy Impact Unnotched 3.30 J/cm² - NB
15.7 ft-lb/in² - NB
Average value: 3.65 J/cm² Grade Count:52
2.20 J/cm² - NB
<br>@Temperature -30.0 - -20.0 °C
10.5 ft-lb/in² - NB
<br>@Temperature -22.0 - -4.00 °F
Average value: 2.85 J/cm² Grade Count:56
Charpy Impact, Notched 0.400 - 7.50 J/cm²
1.90 - 35.7 ft-lb/in²
Average value: 4.77 J/cm² Grade Count:111
0.400 - 5.50 J/cm²
<br>@Temperature -30.0 - 0.000 °C
1.90 - 26.2 ft-lb/in²
<br>@Temperature -22.0 - 32.0 °F
Average value: 2.45 J/cm² Grade Count:64
Gardner Impact 43.0 - 54.0 J
31.7 - 39.8 ft-lb
Average value: 48.5 J Grade Count:5
Dart Drop, Total Energy 5.11 - 100 J
3.77 - 73.8 ft-lb
Average value: 56.4 J Grade Count:70
4.86739 - 70.0 J
<br>@Temperature -40.0 - -20.0 °C
3.59000 - 51.6 ft-lb
<br>@Temperature -40.0 - -4.00 °F
Average value: 51.3 J Grade Count:19
Puncture Energy 45.0 - 47.0 J
33.2 - 34.7 ft-lb
Average value: 46.3 J Grade Count:8
55.0 - 58.0 J
<br>@Temperature -30.0 - -30.0 °C
40.6 - 42.8 ft-lb
<br>@Temperature -22.0 - -22.0 °F
Average value: 57.0 J Grade Count:8
Taber Abrasion, mg/1000 Cycles 20.0 - 40.0
20.0 - 40.0
Average value: 31.0 Grade Count:25
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 - 1.00e+17 ohm-cm
1.00e+13 - 1.00e+17 ohm-cm
Average value: 1.18e+16 ohm-cm Grade Count:64
Surface Resistance 1.00e+9 - 6.02e+16 ohm
1.00e+9 - 6.02e+16 ohm
Average value: 2.89e+15 ohm Grade Count:50
Dielectric Constant 2.80 - 3.80
2.80 - 3.80
Average value: 3.17 Grade Count:50
Dielectric Strength 14.0 - 35.0 kV/mm
356 - 889 kV/in
Average value: 22.1 kV/mm Grade Count:49
Dissipation Factor 0.000600 - 0.0300
0.000600 - 0.0300
Average value: 0.00904 Grade Count:47
Arc Resistance 0.000 - 180 sec
0.000 - 180 sec
Average value: 111 sec Grade Count:29
Comparative Tracking Index 100 - 600 V
100 - 600 V
Average value: 420 V Grade Count:54