Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® LW9330 BK851 PBT
(Unverified Data**) Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE350038 BK083 is a 33% glass reinforced, heat stabilized, lubricated, hydrolysis resistant high performance polyamide resin, developed for improved structural performance. It is also a P.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792, ISO 1183 |
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66 Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® 327UVE RD402 Acetal Homopolymer
(Unverified Data**) Delrin® 327UVE RD402 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Informat.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
Asahi Kasei Tenac® LT805 Acetal Homopolymer, Low Friction Grade
(discontinued **) Excellent friction and wear on metals.Applications: Keyboard parts, bearings for office machines, gears.This product is not a part of the standard product line dated 2003. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP CBL36XXC PS LNP* LUBRICOMP* CBL36XXC is a compound based on Polystyrene resin containing 30% Glass Bead and 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL42 PC LNP* Lubricomp* DFL-4042 a compound based on Polycarbonate resin containing 10% Glass Fiber, 20% PTFE. Added features include: Internally Lubricated. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | |
LATI Latiohm 66-07 PD08 G/30 PA66, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36R PA6.12 (Europe-Africa-Middle East) Internally lubricated PA6.12, containing Glass Fiber and PTFE |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 2200F PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP DF006RXQ PC LNP* THERMOCOMP* DF006RXQ is a compound based on Polycarbonate resin containing 30% Glass Fiber. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP ZFM62P PPE+PS LNP* THERMOCOMP* ZFM62P is a compound based on PPE+PS resin containing 10% Glass Fiber, 30% Mical. Added features of this material include: Exceptional Processing. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RX89047 PA 66 LNP* VERTON* RX89047 is a compound based on Nylon 66 resin containing Proprietary Fillers. Added feature of this grade is: Structural. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RX89047 PA 66 (Europe-Africa-Middle East) LNP* Verton* RX89047 is a compound based on Nylon 66 resin. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
Polyram RamTal PMH2003 Polyacetal Homopolymer for Injection Molding General purpose polyacetal homopolymer for injection molding applications, MFI 3.Information provided by Polyram. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
Toyobo VYLOPET® EMC605P PBT/PET Alloy, Anti-microbial Applications: Gas equipment partsFeatures: Good anti-microbialGood appearanceFlame resistantInformation provided by Toyobo. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-87 Compression Molded PPS Compound, 20% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 90/R Flexible PVC, Flame Retardant Sheathing Hydrocarbon resistant |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1184 |
Fainplast Compounds GK 0185/R Flexible PVC, Flame Retardant Sheathing Lead Free Oil and hydrocarbon resistant sheath (90°C) |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 NL XA20 PBT, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | |
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Dry) Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | |
DuPont™ Kapton® 200HN Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General .. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RF-7007 EM HS PA 66 (Asia Pacific) LNP VERTON* RF-7007 EM HS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |