Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Multibase Multi-Pro® 2006 T Polypropylene Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH T4020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPHC TS25020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH T10020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM Data |
Americas Styrenics Styron® 685 Polystyrene
(discontinued **) STYRON® 685 general purpose polystyrene resin is a high heat resin used in consumer electronics and housewares. It offers excellent clarity, good moldability for use in hot runner systems. When use.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | DIN 53479 |
Ineos Nova S-4200 Medium Impact Compact Polystyrene
(discontinued **) Medium impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection molding of technical.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | DIN 53479 |
Ineos Nova S-4600 High Impact Compact Polystyrene
(discontinued **) High impact polystyrene with excellent flow characteristics, a very high toughness and a high elongation. Main application are injection molding of technical parts and housings. For injection mold.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Global ABS-405 FR High Impact, Flame Retardant ABS Information provided by Global Polymers Corporation. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
KKPC Kuhmo GP 100 High Flow GPPS Key features: High-fluidity, high-transparency. Common Uses: Disposable cups, small containersGPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, moldin.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
Ineos ABS Lustran® ABS 650 Injection Molding Grade Lustran® ABS 650 has high impact strength, high flow, and is injection molding grade. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | |
Ineos Styrenics Polystyrene 148G (NAFTA) High heat, easy flow general purpose polystyrene with excellent clarity. Designed for applications requiring a combination of fast processing with good strength and heat resistance.Information prov.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | |
Momentive Performance Materials RTV6708 Translucent Adhesive Sealant, General Purpose Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: General purpose adhesive sea.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Techmer ES Statiblend® 02020 MB Polypropylene, 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 5% Filler by Weight/Unspecified FillerReinforFeatures: ConductiveTPCI# 9117116Information provided by TP Composites, Inc. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Techmer ES Plastiblend® ABS LE BK Availability: North AmericaForms: PelletsFeatures: Low ExtractablesAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P20 Nylon, conditioned Hiprolon® 11ESNNHL P20 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® FN718 NC010A Nylon 66 Zytel® FN718 NC010A is a flexible, plasticizer free modified polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | |
Arkema Group Pebax® MV 1041 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 60 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....)ISO data provided .. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | |
Arkema Group Orgalloy® RS 6000CD Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0339T20L Talc Reinforced |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | |
BASF Procom® T20C 557 Polypropylene Car interior trim panels.Data was collected by ISO methods and provided by BASF. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
A.D. Compound Adene NTFA Homopolymer 20% Talc Filled Polypropylene Information provided by A.D. Compound |
|||
Density | 1.04 - 1.70 g/cc | 0.0376 - 0.0614 lb/in³ | Average value: 1.27 g/cc Grade Count:267 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPHC TS15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Ineos Nova 3510 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | DIN 53479 |
Ineos Nova S-3201 Medium Impact Compact Polystyrene
(discontinued **) Extremely easy flowing medium impact polystyrene, designed for extreme short cycle times for injection molding of household, packaging and toys. The material is provided with external lubricant to .. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Ineos Nova 8049 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High gloss at 60°=95; at 20°C=90, Improved scuff resistance, Custom colorsApplications: Injection molding, Cost effective replacement for some ABS applications, Excellent for applications where hi.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | |
Sax Polymers SAXLAC 835T Acrylonitrile Butadiene Styrene Saxalac 835T is an antistatic, easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested .. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM Data |
Styron Magnum™ 3490 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
Unitika EX-1030 PA6, Conditioned High-impact nylonInformation provided by Unitika Ltd. |