Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Global ABS-405 FR High Impact, Flame Retardant ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Manufacturer Global Polymers Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global ABS-405 FR High Impact, Flame Retardant ABS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D638
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
ASTM D256