Ineos Nova S-4600 High Impact Compact Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos Nova S-4600 High Impact Compact Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High impact polystyrene with excellent flow characteristics, a very high toughness and a high elongation. Main application are injection molding of technical parts and housings. For injection molding generally a lubricated type is used.All mechanical properties measured under standard conditions 50% RH and 23°C.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
DIN 53479
Water Absorption <= 0.10 %
<= 0.10 %
DIN 53495
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 200 °C
10 g/10 min

@Load 11.0 lb,
Temperature 392 °F
DIN 5375/ISO 1133
Mechanical Properties Metric English Comments
Ball Indentation Hardness 62.0 MPa
8990 psi
DIN 53456
Tensile Strength, Ultimate 20.0 MPa
2900 psi
DIN 53455
Elongation at Break 55 %
55 %
DIN 53455
Modulus of Elasticity 1.50 GPa
218 ksi
DIN 53457
Flexural Yield Strength 35.0 MPa
5080 psi
DIN 53452
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
Low Temp; DIN 53453
9.00 kJ/m²
4.28 ft-lb/in²
DIN 53453/ISO 179
Izod Impact, Unnotched (ISO) NB
NB
DIN 53453
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
DIN 53752
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612
Vicat Softening Point 78.0 °C
172 °F
DIN 53460