Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.14 - 1.32 g/cc @Temperature 240 - 250 °C |
0.0412 - 0.0477 lb/in³ @Temperature 464 - 482 °F |
Average value: 1.25 g/cc Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Density | 1.05 - 1.32 g/cc | 0.0379 - 0.0477 lb/in³ | Average value: 1.12 g/cc Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Density | 1.21 - 1.32 g/cc | 0.0437 - 0.0477 lb/in³ | Average value: 1.27 g/cc Grade Count:8 |
Overview of materials for Polycarbonate, Aramid Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Density | 1.26 - 1.32 g/cc | 0.0455 - 0.0477 lb/in³ | ASTM D792 |
Manifattura Cattaneo PEEK Polyetheretherketone Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | Fusor 2002 |
Lord Adhesives Fusor® 2001 / 2002 Urethane Adhesive Fusor® 2001/2002 is a two-part urethane adhesive system used to bond fiberglass reinforced plastics, sheet molded compound, and bulk molded compound to themselves as well as to primed metals.All .. |
|||
Density | 1.20 - 1.32 g/cc | 0.0434 - 0.0477 lb/in³ | 310B Hardener |
Lord Adhesives Fusor® 310 A/B Epoxy Adhesive Lord® 310 adhesive is a modified, thixotropic, two-part epoxy adhesive which bonds well to many types of prepared metals, prepared rubber, urethane, and plastics. Originally formulated for primer.. |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | |
Sibur 140-13A Compound 8/2 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds CTS 75 Flexible PVC, Extrusion Modified with Rubber Gas pipe covering |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 55 Flexible PVC, Injection Molding for Footwear Tennis shoes |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 7516 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 8016 Flexible PVC, Injection Molding for Footwear Technical items for footwear |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds FRT 91 Flexible PVC, Insulation Telephone cables |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 7022 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 85 Flexible PVC, Insulation for High Temperatures Lead Free Operatine temperature 105°C |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 60/FR Flexible PVC, Extrusion Modified with Rubber Profiels UL 94 Classe V1 |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 86/AF Flexible PVC, Extrusion Modified with Rubber Profiels UL 94 Classe V0 |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds PK 85/N Flexible PVC, Lead Free Profiles DOP Free |
|||
Density | 1.30 - 1.32 g/cc | 0.0470 - 0.0477 lb/in³ | ASTM D792 |
Chang Chun Plastic PBT1100L General Purpose PBT Information provided by Dowell Trading Company Ltd. |
|||
Density | 1.30 - 1.32 g/cc | 0.0470 - 0.0477 lb/in³ | ASTM D792 |
Chang Chun Plastic PBT1200M General Purpose PBT Information provided by Dowell Trading Company Ltd. |
|||
Density | 1.314 - 1.32 g/cc | 0.04747 - 0.0477 lb/in³ | relative; d204 |
Oceanchem Group Iso-Propyl Bromide (2-Bromopropane) Molecular Formula: C3H7BrCas No.: 75-26-3Application: Organic SynthesisStorage: The product should be stored in a cool and dry place.Information Provided by Oceanchem Group |
|||
Density | 1.20 - 1.32 g/cc | 0.0434 - 0.0477 lb/in³ | Average value: 1.26 g/cc Grade Count:23 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 5 Flexible PVC, Extrusion Tunnel waterproofing |
|||
Density | 1.15 - 1.32 g/cc | 0.0415 - 0.0477 lb/in³ | Average value: 1.21 g/cc Grade Count:29 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Density | 1.32 - 1.32 g/cc @Temperature 285 - 285 °C |
0.0477 - 0.0477 lb/in³ @Temperature 545 - 545 °F |
Average value: 1.32 g/cc Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |