Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.11 g/cc | 0.0762 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP 9X98026 PA 46 (Europe-Africa-Middle East) LNP* Lubricomp* 9X98026 is a compound based on PA4.6 resin containing Barium Sulfate, PTFE and Carbon Fiber |
|||
Density | 2.11 g/cc | 0.0762 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 4215 PTFE 25% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Density | 2.11 g/cc | 0.0762 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TFM™ 4215 Modified PTFE, 25% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Density | 2.11 - 2.16 g/cc | 0.0762 - 0.0780 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Density | 2.11 - 2.16 g/cc | 0.0762 - 0.0780 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc.. |
|||
Density | 2.11 - 2.16 g/cc | 0.0762 - 0.0780 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re.. |
|||
Density | 2.11 g/cc | 0.0762 lb/in³ | GB/T 1033.1-2008 |
Sichuan Deyang Haton® hFR81 Polyphenylene Sulfide Injection molding, reinforcedInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Density | 2.11 g/cc | 0.0762 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® 1045 Bearing/Seal PTFE Rulon® 1045 is a dull gold material that has an excellent ability to elongate in a flip seal application. Coupled with excellent frictional characteristics, it offers the added benefit of energy .. |
|||
Density | 2.11 g/cc | 0.0762 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® 1337 Bearing/Seal PTFE Rulon® 1337 is a tan material made entirely from FDA compliant components. It has excellent physical properties and is chemically compatible with most chemicals, except concentrated sulfuric acid.. |
|||
Density | 2.11 g/cc | 0.0762 lb/in³ | ASTM D297 |
Vicone High Performance Rubber VicoFluor™ 06FK-BR High Performance Fluoroelastomer Rubber Meets ASTM D2000 fluoroelastomer 60 Durometer. |
|||
Density | 2.11 g/cc | 0.0762 lb/in³ | ASTM D297 |
Vicone High Performance Rubber VicoFluor™ 57FK-GR High Performance Fluoroelastomer Rubber Meets ASTM D2000 fluoroelastomer 75 Durometer. |
|||
Density | 2.11 g/cc | 0.0763 lb/in³ | |
Devcon Plastic Steel® Liquid (B) Epoxy General Repair EpoxyComments: Steel-filled liquid epoxy can be cast over models for accurate detail reproduction when making holding fixtures, light-gauge forming dies and molds. Hardens in about a.. |
|||
Density | 2.11 g/cc | 0.0762 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN SM-K25 PTFE Based on Tarflen SM1 reinforced with 25% coke for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 2.11 - 2.16 g/cc | 0.0762 - 0.0780 lb/in³ | ASTM D1050-68 |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
Density | 2.11 - 2.16 g/cc | 0.0762 - 0.0780 lb/in³ | ASTM D1050-68 |
Arkema Group VOLTALEF® 302 PCTFE VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group |
|||
Density | 2.11 g/cc | 0.0762 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Algoflon® 25CAR PTFE; Petroleum Coke and Graphite
(discontinued **) Data provided by the manufacturer.25 wt.% Petroleum Coke and Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric p.. |
|||
Density | 2.11 g/cc | 0.0762 lb/in³ | |
Pyrotek Pyrocast ZS Refractory Shapes Aggregate Base: Fused SilicaApplicationsTransfer troughs Information provided by Pyrotek. |
|||
Density | 2.11 g/cc | 0.0762 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN SM-K22G3 PTFE Tarflen SM1 reinforced with 22% coke and 3% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |