Sichuan Deyang Haton® hFR81 Polyphenylene Sulfide

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer Sichuan Deyang Chemical Co. Ltd.
Trade Name Haton®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sichuan Deyang Haton® hFR81 Polyphenylene Sulfide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Injection molding, reinforcedInformation provided by Sichuan Deyang Chemical Co., LTD
Physical Properties Metric English Comments
Density 2.11 g/cc
0.0762 lb/in³
GB/T 1033.1-2008
Water Absorption 0.020 %
0.020 %
GB/T 1034-2008
Linear Mold Shrinkage, Flow 0.00010 cm/cm
0.00010 in/in
GB/T 15585-1995
Linear Mold Shrinkage, Transverse 0.00010 cm/cm
0.00010 in/in
GB/T 15585-1995
Mechanical Properties Metric English Comments
Tensile Strength 60.0 MPa
8700 psi
GB/T 1040.2-2006
Flexural Strength 100 MPa
14500 psi
GB/T 9341-2008
Flexural Modulus 17.0 GPa
2470 ksi
GB/T 9341-2008
Thermal Properties Metric English Comments
Melting Point 280 °C
536 °F
GBT/T 19466.3-2004
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
GB/T 1634.2-2004
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Surface Resistivity per Square 2.40e+14 ohm
2.40e+14 ohm
GB/T1410-2006
Dielectric Constant 4.0
4.0
GB/T 1409-2006
Dielectric Strength 18.0 kV/mm
457 kV/in
GB/T1408.1-2006
Dissipation Factor 0.0020
0.0020
GB/T 1409-2006