Material Notes:
Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low surface energy and exceptional dielectric properties. Hyflon® MFA F1540 is a medium-high melt flow rate multi purpose resin with an exceptional stress crack resistance, continuous service temperature up to 225°C and a 13-15 x 10³ cycles flex-life (on a 0.3 mm film, ASTM D2176).Features: Flame Retardant; High ESCR (Stress Crack Resist.); High FlowUses: General Purpose; Wire & Cable ApplicationsAdditional Properties: Crosshead Temperature - 380 to 410 °C; Crystallization Heat - DSC 16.0 to 24.0 J/g; Flange Temperature - 370 to 400 °C; Flex Life - ASTM D2176 4.0E+4 to 6.0E+4 Cycles; Heat of Fusion - DSC 16.0 to 24.0 J/g; Wire Preheat - 120 °CInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 2.11 - 2.16 g/cc
0.0762 - 0.0780 lb/in³
ASTM D792
Melt Flow 8.0 - 18 g/10 min

@Load 5.00 kg,
Temperature 372 °C
8.0 - 18 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 60
55 - 60
ASTM D2240
Tensile Strength at Break >= 25.0 MPa
>= 3630 psi
50 mm/min; ASTM D638
Elongation at Break >= 300 %
>= 300 %
50 mm/min; ASTM D638
Tensile Modulus 0.400 - 0.500 GPa
58.0 - 72.5 ksi
1.0 mm/min; ASTM D638
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
Specific Heat Capacity 0.900 - 1.10 J/g-°C
0.215 - 0.263 BTU/lb-°F
ASTM C351
Thermal Conductivity 0.200 W/m-K

@Temperature 40.0 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 104 °F
ASTM C177
Melting Point 265 - 275 °C
509 - 527 °F
DSC
Crystallization Temperature 255 - 265 °C
491 - 509 °F
Peak; ASTM D3418
Flammability, UL94 V-0
V-0
Oxygen Index 95 %
95 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+17 ohm-cm
>= 1.00e+17 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+17 ohm
>= 1.00e+17 ohm
ASTM D257
Dielectric Constant 2.0

@Frequency 100000 Hz
2.0

@Frequency 100000 Hz
ASTM D150
2.0

@Frequency 50.0 Hz
2.0

@Frequency 50.0 Hz
ASTM D150
Dielectric Strength 35.0 - 40.0 kV/mm

@Thickness 1.00 mm
889 - 1020 kV/in

@Thickness 0.0394 in
ASTM D149
Dissipation Factor <= 0.00050

@Frequency 100000 Hz
<= 0.00050

@Frequency 100000 Hz
ASTM D150
<= 0.00050

@Frequency 50.0 Hz
<= 0.00050

@Frequency 50.0 Hz
ASTM D150
Processing Properties Metric English Comments
Zone 1 240 - 290 °C
464 - 554 °F
Zone 2 270 - 320 °C
518 - 608 °F
Zone 3 300 - 360 °C
572 - 680 °F
Zone 4 330 - 380 °C
626 - 716 °F
Zone 5 340 - 390 °C
644 - 734 °F
Adapter Temperature 370 - 400 °C
698 - 752 °F
Melt Temperature 390 - 420 °C
734 - 788 °F
Die Cooling Temperature 390 - 420 °C
734 - 788 °F
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Form Pellets
Processing Technique Extrusion Coating
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved