Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.81 g/cc | 0.0654 lb/in³ | ASTM D792 |
Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-3/GPO-3P. Developed for transit industry where smoke generation and toxicity are of primary concern. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ISO R 1183 |
Multibase Multibatch® MP 52214 Injection Molding HPP. 75% CaCO3, 10%TiO2FilledFine Particle Size.Information provided by Multibase |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | Real Density |
SGL Carbon Group CF 5250 Carbon Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
SGL Carbon Group EK 2240 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
SGL Carbon Group EK 2241 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Tecnoflon® FOR TF 636 Fluoroelastomer TECNOFLON® FOR TF 636 is a medium-low viscosity cure incorporated fluoroelastomer terpolymer designed to provide improved low temperature characteristics. Tecnoflon® FOR TF 636 exhibits the sa.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East) Valox 7062 is Mineral filled PBT injection molding grade. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ASTM D792 |
Plenco 5118 Phenolic, Granular, Compression Molded PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ASTM D792 |
Plenco 5118 Phenolic, Granular, Transfer Molded PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
Zoltek Panex 35® 50k Continuous Tow Commercial Carbon Fiber for Industrial Applications Commercial Carbon Fiber for Industrial Applications |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | Fibre |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/G1094/1000 Fiber: T800H 6K, 5H Satin weave, 290 g/m2Information provided by HexCel |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
Cytec Thornel® T-40 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
Cytec Thornel® T-50 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
Devcon Magic Bond™ Epoxy Putty Emergency Repair ProductsComments: Two-part epoxy putty stick seals leaks and repairs gouges in steel, aluminum, wood, fiberglass, concrete and ceramics. Cures rock-hard and can be painted, sanded,.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
Cytec Thornel® T-50 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ISO 1183 |
Barlog Plastics KEBATER BM240 PBT, 40% mineral reinforced, food grade (PBT+X)-MD40Information provided by BARLOG plastics GmbH. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
A. Schulman ComAlloy Hiloy® 422 Heavy Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.40% Heavy Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.81 - 1.85 g/cc | 0.0654 - 0.0668 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 83/M Flexible PVC, Extrusion Covering copper pipes |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ISO 1183 |
LATI LARAMID CE/60 60% Mineral Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**) Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s.. |
|||
Density | 1.81 g/cc @Temperature -120 °C |
0.0654 lb/in³ @Temperature -184 °F |
|
3M Novec™ 7000 Engineered Fluid 3M™ Novec™ 7000 Fluid unique properties make it useful as a low temperature, heat transfer fluid for cooling reactors in pharmaceutical & chemical processing. It's also ideal for low temperature a.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Amodel® AF-1145 V0 Polyphthalamide (PPA) Resin, 45% Glass Reinforced, Dry As Molded
  AMODEL AF-1145 V0 is a 45% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high heat distortion temperature, high tensile strength and flexural modulus. The material is rela.. |