Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IE7010X X-Ply Cross-Ply Polypropylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IE7020 Unitape Unidirectional Polyethylene-Glass Composite Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IE7020X X-Ply Cross-Ply Polyethylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IS7015X X-Ply Cross-Ply Polypropylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous S-Glass (ThermoPro-S™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK608 BK509 PBT
(Unverified Data**) Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
Lanxess Pocan® DP BF 4232 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 3452 PEI (Europe-Africa-Middle East) 45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. Resin is RoHS compliant. UL94 V0 and 5VA listing in recognized colors. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-4-240BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | GB/T 1033.1-2008 |
Sichuan Deyang Haton® hGR302 PPS / F4 Polyphenylene Sulfide Injection molding, anti-frictionInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
Techmer ES Plaslube® J-1850/30/TF/15 PBT, 30% GFR, 15% PTFE |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp JF008 PES LNP* Thermocomp* JF008 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp JF008 PES LNP* Thermocomp* JF008 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP OCF62 PPS - Branched LNP* THERMOCOMP* OCF62 is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP OCF62E PPS - Branched LNP* THERMOCOMP* OCF62E is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RFZ349XC PA 66 LNP THERMOCOMP* RFZ349XC is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% Milled Glass. Added features of this material include: Flame Retardant. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, DRY Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
SGL Carbon Group Ridurid® V 1640 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)
(Unverified Data**) 45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | Liquid |
3M Novec™ 7300DL Engineered Fluid 3M™ Novec™ 7300DL fluid is a clear, colorless, odorless fluid. A high-purity version of 3M™ Novec™ 7300 fluid, designed for demanding applications such as hard disk lubricant deposition & semico.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
Unitika RUN35-C25 Weather resistant PA6, Conditioned Weather resistant, noncoating, external exposure-compatibleInformation provided by Unitika Ltd. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound BMI molding compound long glass fiber reinforced with excellent mechanical and thermal properties. Especially suited to be used for injection molding.Information provided by Sumitomo Bak North Ameri.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IE7011 ECR Unitape Unidirectional Polypropylene-Glass Composite Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IE7015X X-Ply Cross-Ply Polypropylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp PK0069 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PK0069 is a compound based on PA 6 resin containing Glass Bead, Flame Retardant. Added features include Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |