Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
Polykemi AB SCANMID 6 B12^ F50 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36P PC LNP* Lubricomp* DFL36P is a compound based on Polycarbonate containing 30% Glass Fiber 15% PTFE. Added features include: Exceptional Processing. Internally Lubricated. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | |
H.C. Starck Baymetec® Tantalum Ethoxide |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | |
LATI Latishield 66-13A G/30 PA66, Steel/Glass Fiber Reinforced EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KFI15 ACETAL LNP* LUBRICOMP* KFI15 is a compound based on Acetal containing 25% Glass Fiber, 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KFL32R Acetal Copolymer LNP LUBRICOMP* KFL32R is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE. Added feature of this material is: Easy Release, Wear Resistant. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® IQNH4560 PBT (Asia Pacific) Valox* IQNH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10 LNP* THERMOCOMP* QF0069 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10 (Europe-Africa-Middle East) LNP* THERMOCOMP* QF0069 is a compound based on PA610 resin contaning Glass Fiber, Flame Retardant. Added features include: Flame retardant. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RB00A PA 66 (Europe-Africa-Middle East) 50% glass beads filled Polyamide 66 injection moulding resin. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RX09411H PA 66 LNP* Thermocomp* RX09411H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp WB006 PBT LNP* Thermocomp* WB006 is a compound based on Polybutylene Terephalate resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ASTM D792 |
PlastxWorld CEVIAN® B5536 30% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ASTM D792 |
Plenco 4349 Phenolic, Granular, Transfer Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | Laminate |
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Tape Form Fiber: IM7-12KInformation provided by HexCel |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® TSG-50 PA666-GF50 Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based .. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
Eurostar Staramide AS10 PA66, 50% Glass Bead Reinforced, Injection Molding Staramide AS10 is a 50% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | Side 1, Silicone Property; Arlon SQA-TMS-024 |
Arlon 51586R015H 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
BASF Petra® 7010 WT 7729 15% Glass Filled PET Description: Petra 7010 WT7729 is a 15% glass fiber reinforced, pigmented white injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface .. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
BASF Ultradur B 4040 G6 LS High Speed BK15029 30% Glass Filled PBT/PET |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Conditioned, 50% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Density | 1.56 g/cc @Temperature 23.0 °C |
0.0564 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183/A |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6/6 GF25 FR NAT005 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized, High Flow and Lubri.. |