Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
PolyOne Nymax™ GMF 604 40 UV Black 28 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | |
Plastcom SLOVASTER® B/A GF 30 PBT, 30% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
LATI LATAN 13 K/30 30% Carbon Fiber Reinforced Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® S223-G8U (Cond.) 43% Glass Reinforced Nylon 66 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
Plenco Valite 4100 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific) LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON RX98063 PA 66 (Europe-Africa-Middle East) LNP* STAT-KON* RX98063 is a compound based on PA 66 resin containing Glass Fiber, Stainless Steel Fiber. Added features include; Antistatic. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly LNP* THERMOCOMP* KFB11 is a compound based on Acetal Copolymer resin containing 5% Glass Fiber, 5% Glass Bead. Added features of this material include: Low Warpage, Chemically Coupled. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 (Asia Pacific) LNP* Thermocomp* RF0029S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp SF00A PA12 (Europe-Africa-Middle East) Glass filled Nylon 12This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 (Asia Pacific) Glass filled Nylon 12 |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | D792 |
Zhejiang Juner 301-G0 Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
Polyram RamLloy PFS301G6 ASA/PBT Alloy, 30% Glass Fiber 30% Glass fiber reinforced ASA/PBT alloy for injection molding applications.Information provided by Polyram. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
Chengdu Polyster FH7560 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H7560 and self-made flame retardant material. Flame retardant, high tear resistance. Applications requiring flame retardancy, such as wires, cables and optical fiber.Information provided by.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® S223-HM8 Nylon 66-40% Mineral Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® PLS FR95G15DH2 BK269 Nylon 6 15% Glass Reinforced Flame Retardant Heat Stabilized Polyamide Zytel PLSFR95G15DH2 BK269 is 15% glass reinforced flame retardant black PA using SHIELD Technology only from DuPont exceptional resista.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
Eurostar Star L PA6 30V D51 PA6, Glass Filled, Injection Molding Star L PA6 30V D51 is a PTFE Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D1505-85 |
DuPont Teijin Films Melinex® ST339 Polyester Film, 380 Gauge Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A.. |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 80 Flexible PVC, Sheathing General purposes |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
Eurostar Starflam RF0077P PA66/6, 35% Glass Filled, Injection Molded Starflam RF0077P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1007Z270EM)Information provided by Polym.. |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 22 Halogen Free PVC Sheathing; standard grade for power and special cables |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 88/1 Flexible PVC, Flame Retardant Sheathing Operating temperature 105°C |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 4024 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Insulation and sheathing, improved processabilityInformation provided by Fainplast Compo.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
BASF Ultramid® SEGM35 H1 BK 6259 40% Glass/Mineral Filled PA6 (Conditioned) Description: Ultramid SEGM35 H1 BK6259 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compar.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
BASF Ultramid® B3GM35 BKQ642 23220 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid B3GM35 BKQ642 23220 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds AP 92 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RVN17SXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RVN17SXS is a compound based on PA 66 resin containing Long Glass Fiber, MoS2. Added features include; Wear Resistant. |
|||
Density | 1.48 - 1.79 g/cc | 0.0535 - 0.0647 lb/in³ | Average value: 1.64 g/cc Grade Count:22 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |