| Category | Polymer , Thermoplastic , ASA Polymer , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + ASA Blend, Glass Fiber Reinforced |
| Manufacturer | Polyram |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polyram RamLloy PFS301G6 ASA/PBT Alloy, 30% Glass Fiber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.0016 cm/cm | 0.0016 in/in | ISO 2577 |
| Melt Flow | 15 g/10 min <br>@Load 2.16 kg,<br> Temperature 275 °C |
15 g/10 min <br>@Load 4.76 lb,<br> Temperature 527 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 130 MPa | 18900 psi | ISO 527 |
| Elongation at Break | 3.0 % | 3.0 % | ISO 527 |
| Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527 |
| Flexural Strength | 190 MPa | 27600 psi | ISO 178 |
| Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
| Izod Impact, Notched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | ISO 180 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | ISO 11357 |
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 170 °C | 338 °F | ISO 75 |
| Flammability, UL94 | HB <br>@Thickness 3.00 mm |
HB <br>@Thickness 0.118 in |
|
| Flame Spread | 13.3 mm/min | 0.524 in/min | FMVSS302 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 3.7 <br>@Frequency 1.00e+6 Hz |
3.7 <br>@Frequency 1.00e+6 Hz |
IEC 60250 |