Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultramid® SEGM35 H1 BK 6259 40% Glass/Mineral Filled PA6 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® SEGM35 H1 BK 6259 40% Glass/Mineral Filled PA6 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Ultramid SEGM35 H1 BK6259 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G HS BK-106. In parts containing cross sections, significant pressure drops are encountered during filling.Applications: Mirror housings, rear liftgate handles and luggage rack components.Information provided by BASF
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.90 %
0.90 %
24 Hours; ISO 62
1.6 %
1.6 %
50% RH; ISO 62
5.7 %
5.7 %
Saturation; ISO 62
Processing Properties Metric English Comments
Melt Temperature 270 - 295 °C
518 - 563 °F
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Color BK 6259
Commercial Status North America