Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
Polykemi AB POLYform POM C M140 TF2 Polyoxymethylene, Modified Information provided by Polykemi AB |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
Asahi Kasei Tenac® 2013A Acetal Homopolymer, UV Stabilized
(discontinued **) Similar to 3013A, but higher in molecular weight.Applications: Pipe fittings, rollers, exterior automotive parts.This product is not a part of the standard product line dated 2003. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP CBL36XXC PS LNP* LUBRICOMP* CBL36XXC is a compound based on Polystyrene resin containing 30% Glass Bead and 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | |
LATI Latiohm 66-07 PD08 G/30 PA66, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP UCL36ASP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UCL36ASP is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 2210F PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
Techmer ES Luriblend® POM CO AF15 Availability: North AmericaForms: PelletsAdditive: Aramid Resin Lubricant(15%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV007E PA 66 (Europe-Africa-Middle East) LNP* Verton* RV007E is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
Unitika TERRAMAC TE-8210 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | DIN 53479 |
Polyram RamTough PZ300G6 Polycarbonate, 30% Glass Fiber 30% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | |
DuPont™ Kapton® 300HN Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® 127UVE RD402 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 127UVE RD402 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers pigmented red with very low .. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® 300CP BK642 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® 527UVE RD402 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 527UVE RD402 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers pigmented red with very .. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® PC690 NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC690 is a low viscosity acetal homopolymer developed for parts requiring high precision molding in the healthcare indus.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
Eurostar Star L POM D36 POM, Injection Molded Star L POM D36 is Molybdenum Disulfide Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® 100PE NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE NC010 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
Eurostar Staramide PF007 PA6, 35% Glass Fiber Filled, Injection Molded Staramide PF007 is a 35% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 92/3 Flexible PVC, Insulation for High Temperatures Lead Free Operatine temperature 105°C |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | |
Arkema Group Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Dry) Designation ISO 1874-PA12,MHLR,16-020,GB50Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent.Goo.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARNOFORM 300 TF POM Tribological modified grade low level addition of PTFE, which lower coefficient of friction and wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform.. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG311DP is a medium-high viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications .. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
Polyplastics Duracon® EB-08 Acetal Co-polymer (POM), Conductive, Antistatic DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | |
LATI Later 4-V0 PBT, Flame Retardant Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L.. |
|||
Density | 1.42 - 1.44 g/cc | 0.0513 - 0.0520 lb/in³ | ASTM D792 |
Chang Chun Plastic PBT2100 Fire Retardant PBT Information provided by Dowell Trading Company Ltd. |
|||
Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |