Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
Density | 1.37 - 1.65 g/cc | 0.0495 - 0.0596 lb/in³ | Average value: 1.53 g/cc Grade Count:11 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | |
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | |
LATI Lapex A PES Polyether Sulfone (PES). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | |
LATI Latilub 87/28-15T K/20 PC, 20% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG-K is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: Thi.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP KA000 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KA000 is a compound based on Acetal Copolymer resin containing Aramid Fiber, Proprietary Lubricant. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 1100F PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ajedium™ Films -- Veradel® PES 201 NT Polyethersulfone (PESU) Veradel® PES 201 NT polyethersulfone is a tough, high-strength thermoplastics that are suitable for continuous use up to 356°F (180°C). Veradel® film is resistant to oxidation and hydrol.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
Techmer ES Electrablend® POM C BK Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive and CopolymerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Veradel® A-304P Polyethersulfone (PESU) Veradel® A-304P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles.PESU offers excellen.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0137 S2 Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp PF006 PA 6 (Asia Pacific) Nylon 6 compound containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RF006S PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF006S is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | OSTM059 |
Solvay BRICORR® 75 TETRAKIS(HYDROXYMETHYL)PHOSPHONIUM SULPHATE (THPS) Bricorr 75 contains the active ingredient tetrakishydroxylmethyl phosphonium sulphate.Identification: TETRAKIS(HYDROXYMETHYL)PHOSPHONIUM SULPHATE (THPS)CAS: 55566-30-8Available in: Asia Pacific, Eur.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Asia Pacific) Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF33 L NAT024 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: Natural ColorTPCI# 8221102Informatio.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RC00A PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC00A is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
Solvay TECHNYL® 2412GHF6 PA66, 33% glass fiber, Conditioned Description: Polyamid 66, reinforced with 33% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF6 is used in all sectors of indu.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | DIN 53479 |
Polyram PlusTek PB300G33 Nylon 6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | dry; ISO 1183 |
DSM Novamid® 1010G30 NA PA6-GF30 30% Glass Reinforced, Injection Molding, Easy Molding Grade, High Flow |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® FE270050 BK099 Nylon 66
(Unverified Data**) 30% Glass/Mineral Reinforced Polyamide 66Information provided by DuPont Performance Polymers |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
Eurostar Staramide BT6 PA6, 30% Mineral Filled, Injection Molded Staramide BT6 is a 30% Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 039/4 Halogen Free PVC Sheathing, insulation; high flexibility |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Dry) Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | |
A. Schulman ComAlloy Lubrilon® 610 Nylon 6, Carbon Fiber/PTFE Reinforced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | |
Zoltek Pyron® Plain Weave Fabric Oxidized Pan Fiber Oxidized Pan FiberApplications include: Industrial Flame and Thermal Insulation |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D-792 |
Sumitomo Bakelite North America FM 1132P Cellulose Reinforced Phenolic Novolac FM 1132P is a two-stage phenolic molding compound reinforced with cellulose in pellet form. FM-1132P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-10. (Replaces Militar.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
Kuraray Genestar™ G1300A-M41 Nylon, 30% Glass Filled Glass reinforced injection grade. Main Features:Chemical resistanceHeat resistanceExamples of applications:Gears and bearing retainersIntercooler tank and turbo duct pipe |