Material Notes:
Sheathing, insulation; high flexibility
Physical Properties Metric English Comments
Density 1.37 - 1.41 g/cc
0.0495 - 0.0509 lb/in³
IEC 60811
Melt Index of Compound 13 g/10 min

@Load 21.6 kg,
Temperature 150 °C
13 g/10 min

@Load 47.6 lb,
Temperature 302 °F
Fainplast
Mechanical Properties Metric English Comments
Hardness, Shore D 38 - 44
38 - 44
IEC 60811
Tensile Strength at Break 11.0 MPa
1600 psi
IEC 60811
Elongation at Break 260 %
260 %
IEC 60811
Thermal Properties Metric English Comments
Oxygen Index 31 %
31 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm

@Temperature 20.0 °C
1.00e+15 ohm-cm

@Temperature 68.0 °F
ASTM D257