Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Ajedium™ Films -- Veradel® PES 201 NT Polyethersulfone (PESU)

Category Polymer , Film , Thermoplastic , Polyethersulfone (PES)
Manufacturer Solvay Specialty Polymers
Trade Name Ajedium™ Films -- Veradel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ajedium™ Films -- Veradel® PES 201 NT Polyethersulfone (PESU).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Veradel® PES 201 NT polyethersulfone is a tough, high-strength thermoplastics that are suitable for continuous use up to 356°F (180°C). Veradel® film is resistant to oxidation and hydrolysis and withstand prolonged exposure to high temperatures and repeated sterilization. Veradel® 201 NT polyethersulfone films are highly resistant to mineral acids, alkali and salt solutions. Their resistance to detergents and hydrocarbon oils is good, but they will be attacked by polar solvents such as ketones, chlorinated hydrocarbons, and aromatic hydrocarbons. Electrical properties of Veradel® PES films are stable over a wide temperature range and after immersion in water or exposure to high humidity.Features: Acid Resistant; Alkali Resistant; E-beam Sterilizable; Food Contact Acceptable; Good Sterilizability; Good Toughness; High Heat Resistance; High Strength; Hydrolysis Resistant; Oxidation Resistant; Radiation (Gamma) ResistantUses: Appliance Components; Automotive Electronics; Batteries; Electrical Parts; Electrical/Electronic Applications; Food Service ApplicationsAdditional Properties: Area Factor - 142 ft²/lb/mil; Tear Resistance - ASTM D1004 1160 J/cmInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ISO 62
Thickness 50.0 microns
1.97 mil
As Tested
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 71.3 MPa
10300 psi
ASTM D882
Film Tensile Strength at Yield, TD 71.4 MPa
10400 psi
ASTM D882
Film Elongation at Break, MD 140 %
140 %
ASTM D882
Film Elongation at Break, TD 140 %
140 %
ASTM D882
Film Elongation at Yield, MD 7.7 %
7.7 %
ASTM D882
Film Elongation at Yield, TD 7.5 %
7.5 %
ASTM D882
Secant Modulus, MD 2.10 GPa
305 ksi
ASTM D882
Secant Modulus, TD 2.09 GPa
303 ksi
ASTM D882
Dart Drop Test 390 g
0.860 lb
ASTM D1709
Film Tensile Strength at Break, MD 66.3 MPa
9620 psi
ASTM D882
Film Tensile Strength at Break, TD 65.8 MPa
9540 psi
ASTM D882
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
Unannealed; ASTM D648
Oxygen Index 39 %
39 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 1000 Hz
3.5

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 180 kV/mm
4570 kV/in
ASTM D149
Dissipation Factor 0.0010

@Frequency 1000 Hz
0.0010

@Frequency 1000 Hz
ASTM D150
Compliance Properties Metric English Comments
FDA Yes
Yes
NSF Yes
Yes
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.1655
Availability Asia Pacific
Europe
Latin America
North America
Color Yellow
RoHS Compliance RoHS Compliant