Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Pomalux® 25% GF Acetal Copolymer 25% Glass Filled

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 30% Glass Fiber Reinforced
Manufacturer Westlake Plastics
Trade Name Pomalux®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Pomalux® 25% GF Acetal Copolymer 25% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining parts with complex geometries. It is a good choice for many bearing and wear applications since it has a low coefficient of friction and wears well in both wet and dry environments. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Water Absorption 0.29 %
0.29 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D7852
Tensile Strength, Yield 110 MPa
16000 psi
ASTM D638
Tensile Modulus 8.27 GPa
1200 ksi
ASTM D638
Flexural Modulus 7.24 GPa
1050 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 161 °C
322 °F
ASTM D648