Thermal Properties Metric English Comments
CTE, linear 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
Aremco Aremco-Bond™ 855 Epoxy Adhesive  (discontinued **)
High performance epoxy for specialty bonding and potting applications to 350ºF (175°C). Can be applied to a myriad of substrates, offering exceptional chemical, electrical, and mechanical properti..
CTE, linear 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ravago Manufacturing Americas Hylon® N2017STHL Nylon 6 (DAM)
Information provided by Ravago.
CTE, linear 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
ITW Devcon Metal Repair Titanium Putty, Grey
Information provided by ITW Devcon
CTE, linear 39.6 µm/m-°C

@Temperature 22.8 - 260 °C
22.0 µin/in-°F

@Temperature 73.0 - 500 °F
ASTM E831
Saint-Gobain Meldin® 7021 CM Compression Molded Graphite Filled Polyimide
Melidin® 7021 CM is a self-lubricating compression molded polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best fo..
CTE, linear 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Pomalux® 25% GF Acetal Copolymer 25% Glass Filled
Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining par..
CTE, linear 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Tempalux® CN-F Polyetherimide (conductive)
Non-sloughing carbon-fiber filled material which is extremely strong and stiff, has excellent dimensional stability, and high temperature resistance to 415F. This material has broad chemical resist..
CTE, linear 39.6 µm/m-°C
22.0 µin/in-°F
ASTM C531
Chesterton ARC 897 Fine Grade Sliding Wear Compound
Description: ARC 897 is an advanced ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a t..
CTE, linear 39.6 µm/m-°C
22.0 µin/in-°F
ASTM C531
Chesterton ARC BX2 Contractor Grade Fine Sliding Wear Compound
Description: ARC BX2 is an advanced contractor grade ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It ..
CTE, linear 39.6 µm/m-°C
22.0 µin/in-°F
CMT Materials CTB 44 Composite Toolboard High Temperature
CTB-44 is manufactured by CMT Materials for a wide variety of vacuum forming applications. It is suitable for use up to 2500F (1210C). CTB-44 utilizes a copolymer base material and smaller cell st..
CTE, linear 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylene® P6-43FG-0410 43% Glass Fiber Reinforced, Heat and UV Stabilized
Information provided by Asahi Thermofil
CTE, linear 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylene® P6-30FG-1804 30% Glass Fiber Reinforced, Heat and UV
Information provided by Asahi Thermofil
CTE, linear 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Stat-Tech™ RA-06CF-07GF/000 EM Polyarylsulfone - 7% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications - Flow Enhanced Grade
Data provided by PolyOne.
CTE, linear 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Stat-Tech™ RA-06CF-09GF/000 Polyarylsulfone - 9% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications &a
Data provided by PolyOne.
CTE, linear 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Stat-Tech™ RA-06CF-09GF/000 EM Polyarylsulfone - ESD Applications - Flow Enhanced Grade  (discontinued
Data provided by PolyOne.
CTE, linear 39.6 - 77.0 µm/m-°C
22.0 - 42.8 µin/in-°F
Average value: 58.0 µm/m-°C Grade Count:5
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive