Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
PolyOne LubriOne™ NL-30GF/15T Black Polyamide 612 (Nylon 612) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
PolyOne Nymax™ GMF 604 40 UV Black 115 1 X 1 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Nylene® 9533 , 33% Glass Reinforced Nylon 6/12 Description: Nylene® 9533 is a 33% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resou.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Nylene® Norpex® AX30GF , 30% Glass Reinforced Polyphenylene Ether Description: Norpex® AX30GF is a 30% glass fiber reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
PolyOne Trilliant™ HC HC3220-0030 RS Natural Polycarbonate (PC) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR15 MF25 Glass/Mineral Filled Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Polymer Resources TPSF-FRG30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1240MHL BK Nylon 6/6 Available in North America Filler: Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated, Low Warpage and Heat StabilizedRoHS CompliantForm: Pellets Processing .. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Polymer Resources PPX-FRG30 Modified PPO, UL 94 V-1, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
PolyOne Nymax™ GF 1880 33 HS NATURAL Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedHeat StabilizedMolded Test Bars: (Dry as molded:Information provided by PolyOne Corporation. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES Electrablend® PA12 CF13 L 13% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 13% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and lubricatedInformation provided by TP Composi.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES Electrafil® J-3/CF/10 Nylon 6, 10% Carbon Fiber Reinforced |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedUL Fil.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES HiFill® PP CO GF43 CC 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Clariant Renol PA2SP0007HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF25 FR 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightUL File Number: E157318TPCI# 9085101Information provided by TP Composites, Inc. |