Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® MRGF25/15 42H-NBK1 40% Mineral/Glass Fiber Reinforced Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MRGF25/15 42H-NBK1 40% Mineral/Glass Fiber Reinforced Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Mineral/Glass Fiber Reinforced Nylon 6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183-87
Filler Content 40 %
40 %
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
ISO 527-93
Elongation at Break 2.2 %
2.2 %
ISO 527-93
Flexural Strength 170 MPa
24700 psi
ISO 178-93
Flexural Modulus 11.0 GPa
1600 ksi
ISO 178-93
Izod Impact, Notched (ISO) 5.50 kJ/m²
2.62 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-93