Wellman Wellamid® GFX1356-BK01 20% Glass Fiber Reinforced, Lubricated Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GFX1356-BK01 20% Glass Fiber Reinforced, Lubricated Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Glass Fiber Reinforced, Lubricated Nylon 6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ISO 1183-87
Filler Content 20 %
20 %
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa
18100 psi
ISO 527-93
Elongation at Break 2.5 %
2.5 %
ISO 527-93
Flexural Strength 185 MPa
26800 psi
ISO 178-93
Flexural Modulus 6.30 GPa
914 ksi
ISO 178-93
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-93
Users viewing this material also viewed the following: