Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.30 GPa | 914 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 6 GF 25 Polyamide 6, 25% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 25% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | |
Plastcom SLOVALEN PC 69 GF 40 PP, 40% glass beads, mod. of mech. properties FeaturesModified copolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. A.. |
|||
Flexural Modulus | 6.30 - 44.8 GPa | 914 - 6500 ksi | Average value: 21.8 GPa Grade Count:8 |
Overview of materials for Phenolic, Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values .. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
Grupo Repol Dinalon® B1S25 G30XV0 30% Glass Reinforced, V-0 Rated Nylon 6 Mechanical properties are for dry as molded samples.Information provided by Grupo Repol. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KFI16 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFI16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Silicone. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East) VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 LNP* STAT-KON* RFD02 is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific) LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AF006XXZ ABS (Europe-Africa-Middle East) LNP* Thermocomp* AF006XXZ is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX99077 PC (Europe-Africa-Middle East) LNP* Thermocomp* DX99077 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Non-.. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MCR13S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MCR13S is a compound based on Polypropylene resin containing Carbon Fiber, Barium Sulfate. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-.. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RFB33 PA6.6 (Europe-Africa-Middle East) LNP*THERMOCOMP* RFB33 is a compound based on PA66 resin containing Glass Bead, Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
Polyplastics FR-PET® C3015FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178-93 |
Wellman Wellamid® GF1685-WBK1 Nylon 6, 20% Glass Fiber Reinforced All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178-93 |
Wellman Wellamid® GF20-60 XE-BKDX9 Nylon 6, 20% Glass Fiber Reinforced Chrysler DX9 color matchedAll information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178-93 |
Wellman Wellamid® GFX1356-BK01 20% Glass Fiber Reinforced, Lubricated Nylon 6 Description: Glass Fiber Reinforced, Lubricated Nylon 6Information provided by Wellman. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
Polyplastics FR-PET® B3015FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam PX06011 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06011 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding Resin (also known as Starflam PF1005Z222)Information provided by Eurosta.. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
Eurostar Starpylen MCR13S PP, 15% Carbon Fiber Filled, Injection Molded Starpylen MCR13S is a 15% Carbon Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | cond; ISO 178 |
DSM EcoPaXX® Q-HG6 PA410-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
BASF Petra® 7010 BK 5830 15% Glass Filled PET Description: Petra 7010 BK5830 is a 15% glass fiber reinforced, pigmented black injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface .. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | Wet; ASTM D790 |
Asahi Kasei Leona® 14G33 33% Glass Filled Nylon 66 Enhanced strength and stiffness; with 33% GF. Superior heat aging resistance, fatigue resistance, and creep resistance.Applications:Mechanical and electrical parts, engine mounts and other under-the.. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP JF004L PES LNP* THERMOCOMP* JF004L is a compound is based on Polyethersulfone containing 20% Glass Fiber. Characteristics of this grade is: Low Extractible |