Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Unifrax Fiberfrax® Duraboard® 2600 Ceramic Fiber Board

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Unifrax I LLC
Trade Name Fiberfrax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax Fiberfrax® Duraboard® 2600 Ceramic Fiber Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard products offer low thermal conductivity, high temperature stability, uniform density, and excellent resistance to thermal shock and chemical attack.Duraboard 2600 insulation is a high-temperature insulating board designed to provide high stability at elevated temperatures. This capability is achieved by manufacturing a board formulated with a blend of Fiberfrax® alumina-silica fibers and Fibermax®, Unifrax's patented polycrystalline mullite fibers. This unique formulation controls thermal shrinkage to a level less than 1.0% after 168 hours at 2450°F / 1343°C.Description: Formed from a special blend of Fiberfrax alumina-silica fibers and Fibermax® Mullite fibers. These boards give high stability at temperatures up to 2450°F / 1343°C.Information Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.224 g/cc
0.00810 lb/in³
Nominal
Loss On Ignition 4.0 - 6.0 %
4.0 - 6.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000448 GPa
0.0650 ksi
Fired (24 hrs at cont. use)
0.00103 GPa
0.150 ksi
Green (typ.)
Compressive Strength 0.124 MPa
18.0 psi
10% Deformation; Fired
0.124 MPa
18.0 psi
15% Deformation; Fired
0.131 MPa
19.0 psi
5% Deformation; Fired
0.152 MPa
22.0 psi
5% Deformation; Green
0.172 MPa
25.0 psi
10% Deformation; Green
0.186 MPa
27.0 psi
15% Deformation; Green
Thermal Properties Metric English Comments
Melting Point 1816 °C
3301 °F
Maximum Service Temperature, Air 1343 °C
2449 °F
Recommended Operating Temperature
Shrinkage <= 2.0 %

@Time 86400 sec
<= 2.0 %

@Time 24.0 hour
at Recommended Operating Temperature
Electrical Properties Metric English Comments
Dielectric Strength 1.06 kV/mm
27.0 kV/in
Descriptive Properties Value Comments
Color Cream
Fiberfrax® Fibers (%) 75
Fibermax® Fibers (%) 25
Temperature Grade (°C) 1427