Greene Tweed Arlon® 1286 Polyketone, Carbon Filled

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Greene Tweed
Trade Name Arlon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed Arlon® 1286 Polyketone, Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Greene Tweed offers precision plastic components for a variety of demanding semiconductor applications. These components are made from a full range of high-performance plastic materials including Arlon® 1286, which is ideal for applications requiring exceptionally high physical properties, wear resistance and chemical compatibility.Applications:CMP retainer ringsGuidesSupportsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Water Absorption 0.10 %
0.10 %
24 hrs, 73°F
Mechanical Properties Metric English Comments
Hardness, Shore D 93
93
ASTM D2240
Tensile Strength at Break 260 MPa
37700 psi
ASTM D368
Elongation at Break 1.3 %
1.3 %
ASTM D638
Flexural Strength 392 MPa
56800 psi
ASTM D790
Flexural Modulus 27.9 GPa
4040 ksi
Flexural 0.5% Secant Modulus; ASTM D790
Shear Strength 95.98 MPa
13920 psi
Transverse; ASTM D732
135.6 MPa
19660 psi
Axial; ASTM D732
Coefficient of Friction, Dynamic 0.14
0.14
PV=12600 psi-ft./min.; ASTM G77
Thermal Properties Metric English Comments
CTE, linear 0.900 µm/m-°C

@Temperature <=149 °C
0.500 µin/in-°F

@Temperature <=300 °F
ASTM E228
2.16 µm/m-°C

@Temperature >=149 °C
1.20 µin/in-°F

@Temperature >=300 °F
ASTM E228
Deflection Temperature at 1.8 MPa (264 psi) 316 °C
600 °F
Descriptive Properties Value Comments
Color Black