Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass and Mineral Filled BMC
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where high surface hardness is required.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 2.07 - 2.27 g/cc
0.0748 - 0.0820 lb/in³
Molded
Linear Mold Shrinkage 0.0022 - 0.0042 cm/cm
0.0022 - 0.0042 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 60 - 70
60 - 70
Tensile Strength 49.6 - 63.4 MPa
7200 - 9200 psi
Flexural Strength 103 - 131 MPa
15000 - 19000 psi
Flexural Modulus 7.58 - 8.96 GPa
1100 - 1300 ksi
Compressive Strength 135 - 163 MPa
19600 - 23600 psi
Izod Impact, Notched 2.30 - 2.40 J/cm
4.30 - 4.50 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 218 - 260 °C
425 - 500 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength 13.2 - 15.2 kV/mm
335 - 385 kV/in
short time
Arc Resistance 181 sec
181 sec
Processing Properties Metric English Comments
Processing Temperature 143 - 171 °C
290 - 340 °F