Polymer Property : Compressive Strength = 0.186 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.186 - 0.228 MPa
27.0 - 33.0 psi
0.5; ASTM D1056
Monmouth Rubber & Plastics Superbounce 57 NEO/SBR
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.186 MPa
27.0 psi
15% Deformation; Green
Unifrax Fiberfrax® Duraboard® 2600 Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..
Compressive Strength 0.186 MPa
27.0 psi
5% Deformation; Fired
Unifrax Fiberfrax® Duraboard® 350ES Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..